Die Lines on PMMA Sheet: Tracing a Fixed Streak Back to the Lip

Die Lines on PMMA Sheet: Tracing a Fixed Streak Back to the Lip
Profile extrusion: a production part is the only useful reference for a discussion about process drift.

A single longitudinal line that never moves along the sheet width is usually a die-lip condition, not a random scratch from handling.

What the failure looks like on the line

Acrylic rod, sheet and tube are sold on optical quality, where a small internal defect is more visible than a dimensional error.

A PMMA sheet carries one or more fine, straight lines running continuously in the machine direction at a fixed lateral position. The line survives changes to line speed and reappears at the same place after every start-up, which separates it from random handling scratches.

A nick, polished-through edge or adherent deposit on the die lip imprints a persistent ridge or groove on the melt as it leaves the land. Because the defect is fixed to the tool, the streak stays at a constant cross-width position across the whole run. Polishing the lip or refurbishing the land removes it; adjusting melt temperature only changes how strongly the line is visible.

The useful question is not whether the part conforms, but which condition was never written into the specification. On a buyer's specification this distinction matters: a part can measure inside tolerance and still fail in use, because the drawing records geometry while the complaint records behaviour. Die-lip surface finish is usually the first value both sides compare, and it is also the one most often quoted without the conditions attached to it.

The process window that decides it

Four variables move this result more than the rest. The ranges below are illustrative engineering guidance for a first discussion; confirm them on your own tool, material grade and part geometry before they become contract terms.

可変 Typical window What fails outside it
Die-lip surface finish Ra 0.05-0.20 um A rougher or scored lip prints a visible line into the sheet
Lip edge radius 0.1-0.3 mm A chipped or rounded edge leaves a fixed meniscus mark
Melt temperature at die 210-240 C Running cool makes the surface replicate lip damage more sharply
Die service interval 800-1500 h between inspections Extending the interval lets small nicks grow into permanent streaks

Table 1. Starting window for a joint process trial. Values are engineering guidance, not a measured survey.

Die-lip surface finish is typically held at Ra 0.05-0.20 um. A rougher or scored lip prints a visible line into the sheet Record it together with the measurement point and the moment in the cycle; a single number without a location is not a process setting.

Lip edge radius is typically held at 0.1-0.3 mm. A chipped or rounded edge leaves a fixed meniscus mark When this drifts, the symptom usually appears at one cavity, one sheet position or one lane before it appears across the whole batch.

Melt temperature at die is typically held at 210-240 C. Running cool makes the surface replicate lip damage more sharply A change here is cheap during a trial and expensive after tooling release, so treat it as a controlled variable with a documented re-approval.

Die service interval is typically held at 800-1500 h between inspections. Extending the interval lets small nicks grow into permanent streaks Put it on the change-control list, otherwise an unannounced material or setting substitution will be mistaken for ordinary process noise.

Reading the response curve

Die Lines on PMMA Sheet: Tracing a Fixed Streak Back to the Lip: Visible die-line count per width (relative) against Die service time (h, relative)
Figure 1. Left: Visible die-line count per width (relative) against Die service time (h, relative). Right: how audited failures of this type typically split by cause. All plotted values are illustrative engineering guidance, not a measured survey.

The left panel shows visible die-line count per width (relative) as die service time (h, relative) increases: the response rises from 10 to 91 on the illustrative 0–100 scale. The dashed line at 35 marks a proposed acceptance limit, not a universal standard. Move that line only after the test method and the sample plan have been agreed, otherwise two suppliers can both be compliant and still deliver different parts.

Read the shape rather than a single point. A curve that changes quickly near the limit is more sensitive to ordinary process noise than one that approaches it gradually, and that difference should be reflected in how tightly the setting is controlled and how often it is checked.

Where the causes actually sit

The right panel of Figure 1 splits audited failures of this type into five groups. The percentages are illustrative engineering guidance for prioritising an investigation, not a measured survey and not a prediction for your line.

原因 Illustrative share First check
Nicked or scored die lip 34% Mark the lateral position of the streak on a cut sample and re-check after a restart.
Adherent degraded deposit 24% Shut down and inspect the full die lip under oblique light for nicks or deposit.
Worn land edge 18% Compare the two sheet surfaces to confirm the line is on the die side, not a roll.
Low melt temperature at die 14% Polish a small lip area and re-run to see whether the streak disappears.
Over-extended service interval 10% Log the hours since the last die refurbishment against streak count.

Table 2. Cause split and the corresponding first check. Shares are indicative and sum to 100.

Nicked or scored die lip accounts for roughly 34% of the illustrative split. Mark the lateral position of the streak on a cut sample and re-check after a restart. Start here before authorising a material or tooling change, because it is the fastest explanation to confirm or eliminate.

Adherent degraded deposit accounts for roughly 24% of the illustrative split. Shut down and inspect the full die lip under oblique light for nicks or deposit. Start here before authorising a material or tooling change, because it is the fastest explanation to confirm or eliminate.

Worn land edge accounts for roughly 18% of the illustrative split. Compare the two sheet surfaces to confirm the line is on the die side, not a roll. Start here before authorising a material or tooling change, because it is the fastest explanation to confirm or eliminate.

Checks before sign-off

Work through these in order; measuring a later variable before an earlier one hides the cause rather than finding it.

  1. Mark the lateral position of the streak on a cut sample and re-check after a restart.
  2. Shut down and inspect the full die lip under oblique light for nicks or deposit.
  3. Compare the two sheet surfaces to confirm the line is on the die side, not a roll.
  4. Polish a small lip area and re-run to see whether the streak disappears.
  5. Log the hours since the last die refurbishment against streak count.

Keep a retained reference sample beside every result. When a batch is disputed, the comparison that settles it is almost always between the retained part and the current one under the same method, not between either part and a number on a drawing. Record the instrument, the operator, the conditioning time and the position on the part or sheet for each reading.

Writing it into the specification and the evidence pack

No fixed longitudinal streak shall be visible above the agreed limit sample under the specified inspection lighting, with the die-lip condition recorded at the last planned refurbishment.

Write the requirement as a behaviour at a stated condition, not as a brand of material or a machine setting. State the test method, the conditioning, the sample plan and the rule for deciding a pass. Where a document is needed, ask the supplier for documentation that covers the actual construction and check its scope against your own market before approval; a document for the base material alone does not describe the finished part you are buying.

At first-article approval, freeze the drawing revision, the material and colour identification, the process window, the tool and cavity identification, and the inspection method. Any later change to grade, site, tool, or window should trigger a new first article rather than a paper waiver. Keep retained samples from the approved lot and from each production lot so that a future comparison is possible.

Evidence item What it must show
Approved drawing and revision The exact geometry and tolerances the decision applies to
Material and colour identification Grade, supplier, colour reference and any declared recycled content
Process window and change log The agreed settings and any deviation since approval
Inspection record and retained samples Method, conditions, results and a physical reference from the same lot

Table 3. Minimum evidence pack for a first-article decision and a later batch dispute.

The values quoted here are illustrative engineering guidance, not a measured survey. Agree the test method, the sample size and the acceptance rule before comparing numbers across suppliers.

Questions buyers ask

Is this a material problem or a process problem?

A nick, polished-through edge or adherent deposit on the die lip imprints a persistent ridge or groove on the melt as it leaves the land. Because the defect is fixed to the tool, the streak stays at a constant cross-width position across the whole run. Polishing the lip or refurbishing the land removes it; adjusting melt temperature only changes how strongly the line is visible. It is worth separating the two before a supplier changes a grade: hold the material constant for one controlled run, then move one setting at a time. If the symptom follows the setting, the material was never the cause.

Can die-lip surface finish be traded against cycle time?

Only within the window stated in Table 1, and only with a recorded trial. A rougher or scored lip prints a visible line into the sheet A faster cycle that sits outside the window usually moves the failure downstream, where it costs more to find.

What should be recorded at incoming inspection?

Keep the measurement, the method, the sample identity and the conditions together. Mark the lateral position of the streak on a cut sample and re-check after a restart. A result without its conditions cannot be compared with a later batch.

Does a change of PMMA require re-approval?

Treat any change to material grade, tool, site or process window as a change that needs a new first-article decision. For profile extrusion work the drawing alone is not enough; the process route is part of what was approved.

How many samples are enough for a first-article decision?

There is no universal number. Sample across cavities, lanes, sheet positions or reel lengths so that the spread is visible, not just the average. Agree the sample plan and the acceptance rule with the supplier before the trial starts.

What belongs in the evidence pack?

The approved drawing and revision, the material and colour identification, the process window, the inspection method and results, the retained reference samples, and documentation covering the actual construction. Ask the supplier to state the scope of each document and check it against your own market.

Seeing this on a current profile extrusion job?

Send the drawing, the material and grade, the process window you are running, and the point in the cycle or the shelf life where the fault appears. We will help you separate a material question from a process question and a specification question before anyone changes a tool.

Talk to our profile extrusion team

最新の投稿

WhatsApp
フェイスブック
ツイッター
LinkedIn
ピンタレスト
Hi there! I'm John, dad and hero to awesome kid. By day, I'm a plastics manufacturing vet — injection molding, extrusion and vacuum forming — who went from factory floors to technical management. Here to share what I've learned—let's grow together!
jaJA

クイック見積もり

図面および詳細要件を下記までお送りください。

Emial: [email protected]

または下記のお問い合わせフォームにご記入ください: