Polystyrene is the cheapest transparent plastic and the easiest to mould, which keeps it in disposable packaging, display items and appliance liners. Crystal PS gives water-clear parts at very low cost; HIPS adds rubber for toughness and an opaque, uniform surface that takes print and lamination well. Neither survives solvents or high heat, so the application decides.

Custom PS & HIPS Injection Molding — Disposable packaging and clamshells

70 – 85 °CHDT at 1.8 MPa
20 – 45 MPaTensile strength
1.04 – 1.05 g/cm³密度

Typical values for standard moulding grades. Exact figures depend on the specific compound or grade — confirm against your drawing before quoting.

Key properties

プロパティ Typical value
密度 1.04 – 1.05 g/cm³
Tensile strength 20 – 45 MPa
Flexural modulus 2.0 – 3.3 GPa
HDT at 1.8 MPa 70 – 85 °C
Mould shrinkage 0.4 – 0.7 %
Light transmission 88 – 90 % (crystal PS)

Values are typical for unfilled moulding grades at 23 °C unless stated. Glass-filled and specialty grades differ.

Typical applications

  • Disposable packaging and clamshells
  • Point-of-sale display and signage
  • Refrigerator and appliance liners
  • Cosmetic and medical packaging
  • CD cases and media housings

Processing notes

  • Melt 200 – 250 °C, mould 30 – 60 °C. PS processes over a wide window, which is why it is often used for trial shots.
  • Dry 2 h at 70 – 80 °C for optical parts. For packaging grades, drying is usually unnecessary.
  • PS is brittle in thin sections and solvent-sensitive. Avoid contact with adhesives containing ketones or aromatics.
  • For HIPS, specify the rubber content — 5 % and 12 % behave very differently in impact and in surface gloss.
Tooling, not just material. Every material above behaves differently in the tool — shrinkage, gate position, cooling and ejection all change. We review the DFM against the specific grade before the tool is cut, so the first shot is a sample, not a surprise.

Frequently asked questions

Is PS suitable for food packaging?

Yes, in food-contact grades. Crystal PS is common for bakery and produce packaging; HIPS for dairy containers. We supply the migration declaration for the grade used.

Why is PS cheaper than ABS?

Lower polymer cost and a wider processing window, which means shorter cycles and less scrap. Where the part does not need ABS impact strength or heat resistance, PS is the rational choice.

Related materials

← All Injection Molding Solutions

Send us your PS & HIPS drawing

Upload a 3D model or a 2D drawing and we will come back with a DFM review, a tooling cost and a piece price — usually within two working days.

Request a quote

jaJA

クイック見積もり

図面および詳細要件を下記までお送りください。

エミアル:[email protected]

または下記のお問い合わせフォームにご記入ください: