Polypropylene is the lightest of the volume thermoplastics and the cheapest per part once you account for density. It shrugs off acids, bases and most solvents, and a properly gated living hinge will flex a million cycles without cracking. The catch is shrinkage of one to two percent and a tendency to warp — both manageable, but only if the tool is designed for them from the start.

Custom PP Injection Molding — Bottle caps and closures

100 – 110 °CHDT at 0.45 MPa
25 – 40 MPaTensile strength
0.90 – 0.91 g/cm³밀도

Typical values for standard moulding grades. Exact figures depend on the specific compound or grade — confirm against your drawing before quoting.

Key properties

속성 Typical value
밀도 0.90 – 0.91 g/cm³
Tensile strength 25 – 40 MPa
Flexural modulus 1.2 – 1.7 GPa
HDT at 0.45 MPa 100 – 110 °C
Mould shrinkage 1.0 – 2.5 %
Water absorption (24 h) < 0.02 %

Values are typical for unfilled moulding grades at 23 °C unless stated. Glass-filled and specialty grades differ.

Typical applications

  • Bottle caps and closures
  • Food containers and thin-wall packaging
  • Living-hinge lids and flip tops
  • Automotive battery trays and interior panels
  • Chemical tanks and laboratory ware

Processing notes

  • No drying needed in most cases — PP absorbs almost no water. Skip the dryer and save a process step.
  • Melt 200 – 260 °C, mould 20 – 60 °C. A cold mould gives the best gloss and the shortest cycle.
  • Shrinkage of 1.5 % means a 100 mm span moves 1.5 mm. Design ribs and bosses so that differential shrinkage pulls the part flat rather than into a banana.
  • For living hinges, gate so the melt flows across the hinge line, and keep the hinge thin — 0.25 to 0.4 mm — with a sharp entry radius.
Tooling, not just material. Every material above behaves differently in the tool — shrinkage, gate position, cooling and ejection all change. We review the DFM against the specific grade before the tool is cut, so the first shot is a sample, not a surprise.

Frequently asked questions

Why does my PP part warp even though the tool is correct?

Almost always differential shrinkage between a thick boss and a thin wall, or uneven cooling between the two halves. Packing profile and mould temperature balance fix it more often than a tool change does.

Is PP suitable for food contact?

Yes, in a food-contact grade with the appropriate declaration. We supply the migration documentation your market requires, whether that is EU 10/2011 or FDA 21 CFR.

Related materials

← All Injection Molding Solutions

Send us your PP drawing

Upload a 3D model or a 2D drawing and we will come back with a DFM review, a tooling cost and a piece price — usually within two working days.

Request a quote

ko_KRKO

빠른 견적 요청하기

다음을 통해 도면 및 세부 요구 사항을 보내주세요.

Emial: [email protected]

또는 아래 문의 양식을 작성하세요: