Injection moulding: a production part is the only useful reference for a discussion about process drift.

A dark scorch appears at the end of a blind rib in a bearing seat, with a faint fuel-like odour, though melt temperature is within set-point.

What the failure looks like on the line

Industrial moulded parts are usually specified by a drawing and a duty cycle, not by appearance, which is why a dimensionally conforming part can still fail in service.

A brown or black char sits at the blind end of a deep rib where the flow front finishes. The mark is repeatable at the same cavity and the surrounding material looks otherwise normal.

Air and volatiles trapped in a blind pocket are compressed adiabatically as the melt front arrives, raising the gas temperature enough to scorch the polymer, the diesel effect. Inadequate venting at the last-to-fill region prevents escape, and a fast fill leaves no time for the gas to clear. The burn is a local gas-compression phenomenon, distinct from thermal degradation in the barrel.

The useful question is not whether the part conforms, but which condition was never written into the specification. On a buyer's specification this distinction matters: a part can measure inside tolerance and still fail in use, because the drawing records geometry while the complaint records behaviour. Vent depth is usually the first value both sides compare, and it is also the one most often quoted without the conditions attached to it.

The process window that decides it

Four variables move this result more than the rest. The ranges below are illustrative engineering guidance for a first discussion; confirm them on your own tool, material grade and part geometry before they become contract terms.

변수 Typical window What fails outside it
Vent depth 0.02-0.05 mm Too shallow a vent traps gas at the rib end
Injection speed at last fill 15-35 mm/s A fast final front compresses the trapped gas
용융 온도 220-250 C High melt adds volatiles that intensify the scorch
Back pressure 5-10 MPa High back pressure carries more volatiles into the cavity

Table 1. Starting window for a joint process trial. Values are engineering guidance, not a measured survey.

Vent depth is typically held at 0.02-0.05 mm. Too shallow a vent traps gas at the rib end Record it together with the measurement point and the moment in the cycle; a single number without a location is not a process setting.

Injection speed at last fill is typically held at 15-35 mm/s. A fast final front compresses the trapped gas When this drifts, the symptom usually appears at one cavity, one sheet position or one lane before it appears across the whole batch.

용융 온도 is typically held at 220-250 C. High melt adds volatiles that intensify the scorch A change here is cheap during a trial and expensive after tooling release, so treat it as a controlled variable with a documented re-approval.

Back pressure is typically held at 5-10 MPa. High back pressure carries more volatiles into the cavity Put it on the change-control list, otherwise an unannounced material or setting substitution will be mistaken for ordinary process noise.

Reading the response curve

Burn Marks at Blind Ribs in Bearing Seats: Trapped Gas: Burn occurrence (relative index) against Final-stage injection speed (mm/s)
Figure 1. Left: Burn occurrence (relative index) against Final-stage injection speed (mm/s). Right: how audited failures of this type typically split by cause. All plotted values are illustrative engineering guidance, not a measured survey.

The left panel shows burn occurrence (relative index) as final-stage injection speed (mm/s) increases: the response rises from 10 to 93 on the illustrative 0–100 scale. The dashed line at 60 marks a proposed acceptance limit, not a universal standard. Move that line only after the test method and the sample plan have been agreed, otherwise two suppliers can both be compliant and still deliver different parts.

Read the shape rather than a single point. A curve that changes quickly near the limit is more sensitive to ordinary process noise than one that approaches it gradually, and that difference should be reflected in how tightly the setting is controlled and how often it is checked.

Where the causes actually sit

The right panel of Figure 1 splits audited failures of this type into five groups. The percentages are illustrative engineering guidance for prioritising an investigation, not a measured survey and not a prediction for your line.

원인 Illustrative share First check
Blocked or shallow vents 36% Locate the char at the last-to-fill point with a short-shot sequence.
Fast final-stage fill 26% Inspect and measure the vent depth at that cavity position.
Blind rib geometry 18% Reduce final-stage injection speed and compare the next shots.
High melt volatiles 12% Check for blocked or crushed parting-line vents near the rib.
Over-clamping closing vents 8% Compare barrel residence and melt temperature against the set-up sheet.

Table 2. Cause split and the corresponding first check. Shares are indicative and sum to 100.

Blocked or shallow vents accounts for roughly 36% of the illustrative split. Locate the char at the last-to-fill point with a short-shot sequence. Start here before authorising a material or tooling change, because it is the fastest explanation to confirm or eliminate.

Fast final-stage fill accounts for roughly 26% of the illustrative split. Inspect and measure the vent depth at that cavity position. Start here before authorising a material or tooling change, because it is the fastest explanation to confirm or eliminate.

Blind rib geometry accounts for roughly 18% of the illustrative split. Reduce final-stage injection speed and compare the next shots. Start here before authorising a material or tooling change, because it is the fastest explanation to confirm or eliminate.

Checks before sign-off

Work through these in order; measuring a later variable before an earlier one hides the cause rather than finding it.

  1. Locate the char at the last-to-fill point with a short-shot sequence.
  2. Inspect and measure the vent depth at that cavity position.
  3. Reduce final-stage injection speed and compare the next shots.
  4. Check for blocked or crushed parting-line vents near the rib.
  5. Compare barrel residence and melt temperature against the set-up sheet.

Keep a retained reference sample beside every result. When a batch is disputed, the comparison that settles it is almost always between the retained part and the current one under the same method, not between either part and a number on a drawing. Record the instrument, the operator, the conditioning time and the position on the part or sheet for each reading.

Writing it into the specification and the evidence pack

The defined burn-prone region shall be graded against a signed limit sample under fixed lighting; a scorch beyond the sample is rejectable, and vent condition shall be recorded at the agreed tool-maintenance interval.

Write the requirement as a behaviour at a stated condition, not as a brand of material or a machine setting. State the test method, the conditioning, the sample plan and the rule for deciding a pass. Where a document is needed, ask the supplier for documentation that covers the actual construction and check its scope against your own market before approval; a document for the base material alone does not describe the finished part you are buying.

At first-article approval, freeze the drawing revision, the material and colour identification, the process window, the tool and cavity identification, and the inspection method. Any later change to grade, site, tool, or window should trigger a new first article rather than a paper waiver. Keep retained samples from the approved lot and from each production lot so that a future comparison is possible.

Evidence item What it must show
Approved drawing and revision The exact geometry and tolerances the decision applies to
Material and colour identification Grade, supplier, colour reference and any declared recycled content
Process window and change log The agreed settings and any deviation since approval
Inspection record and retained samples Method, conditions, results and a physical reference from the same lot

Table 3. Minimum evidence pack for a first-article decision and a later batch dispute.

None of the figures above should be read as a measured survey. They are engineering guidance for framing a joint trial; confirm them on your own tool, grade and geometry before they become contract terms.

Questions buyers ask

Is this a material problem or a process problem?

Air and volatiles trapped in a blind pocket are compressed adiabatically as the melt front arrives, raising the gas temperature enough to scorch the polymer, the diesel effect. Inadequate venting at the last-to-fill region prevents escape, and a fast fill leaves no time for the gas to clear. The burn is a local gas-compression phenomenon, distinct from thermal degradation in the barrel. It is worth separating the two before a supplier changes a grade: hold the material constant for one controlled run, then move one setting at a time. If the symptom follows the setting, the material was never the cause.

Can vent depth be traded against cycle time?

Only within the window stated in Table 1, and only with a recorded trial. Too shallow a vent traps gas at the rib end A faster cycle that sits outside the window usually moves the failure downstream, where it costs more to find.

What should be recorded at incoming inspection?

Keep the measurement, the method, the sample identity and the conditions together. Locate the char at the last-to-fill point with a short-shot sequence. A result without its conditions cannot be compared with a later batch.

Does a change of industrial require re-approval?

Treat any change to material grade, tool, site or process window as a change that needs a new first-article decision. For injection moulding work the drawing alone is not enough; the process route is part of what was approved.

How many samples are enough for a first-article decision?

There is no universal number. Sample across cavities, lanes, sheet positions or reel lengths so that the spread is visible, not just the average. Agree the sample plan and the acceptance rule with the supplier before the trial starts.

What belongs in the evidence pack?

The approved drawing and revision, the material and colour identification, the process window, the inspection method and results, the retained reference samples, and documentation covering the actual construction. Ask the supplier to state the scope of each document and check it against your own market.

Seeing this on a current injection moulding job?

Send the drawing, the material and grade, the process window you are running, and the point in the cycle or the shelf life where the fault appears. We will help you separate a material question from a process question and a specification question before anyone changes a tool.

Talk to our injection moulding team

Hi there! I'm John, dad and hero to awesome kid. By day, I'm a plastics manufacturing vet — injection molding, extrusion and vacuum forming — who went from factory floors to technical management. Here to share what I've learned—let's grow together!
ko_KRKO

빠른 견적 요청하기

다음을 통해 도면 및 세부 요구 사항을 보내주세요.

Emial: [email protected]

또는 아래 문의 양식을 작성하세요: