Silicone O-Rings: Groove Design, Squeeze and Compression Set

Shallow stainless tray of black silicone O-rings with a compression set jig and a digital caliper on the bench
Silicone O-rings and a compression set jig. Squeeze is what makes the seal, and set is what eventually takes it away.

A seal is a spring, not a plug

An O-ring does not seal by blocking a gap. It seals by being squeezed, and by pushing back against the surfaces that squeezed it. The force it pushes back with is what holds the two faces apart just enough to keep the gap closed, and it is that force, not the rubber itself, that keeps the fluid out.

That reframing matters because it tells you what to measure. A seal fails when the force it pushes back with falls below what the pressure is trying to open. The rubber can be perfectly intact and still fail, because it has taken a set and no longer pushes back.

Silicone is unusually good at staying elastic over a wide temperature range and unusually poor at holding force at high temperature for long periods. That combination makes the squeeze decision more important on silicone than on nitrile, because the material has less reserve.

Squeeze: the number that decides both

Sealing force against squeeze: 12 N per 10 mm of circumference at 10 percent, 21 at 15, 31 at 20, 44 at 25 and 60 at 30. The curve is not linear because the contact width grows with squeeze as well as the stress, so force rises faster than squeeze does.

Compression set over the same range: 8 percent at 10, 11 at 15, 14 at 20, 18 at 25 and 24 at 30. Set is the permanent deformation left after the load is removed, and it rises with squeeze because a more highly strained rubber relaxes more.

So squeeze is the only design variable that buys force and costs life in the same movement. Twenty percent is the usual compromise, and it is a compromise rather than an optimum: it gives about 31 N per 10 mm, which is enough for most static seals, at a set that leaves useful force after a thousand cycles.

Sealing force against squeeze percentage, and compression set against the same squeeze percentage
Sealing force rises from 12 to 60 N per 10 mm between 10 and 30 percent squeeze, while compression set rises from 8 to 24 percent over the same range.

Groove fill: the limit that catches people

Squeeze is only meaningful if there is somewhere for the displaced rubber to go. A groove has a cross-sectional area, the O-ring has a cross-sectional area, and the ratio is the fill. Above about 85 percent fill there is no room left, and the O-ring stops behaving like a spring and starts behaving like a hydraulic fluid.

The failure mode is spectacular. A groove that is over-filled with a low-hardness ring will not seat, the flange will not close to metal-to-metal, and the joint will leak at a torque that should have been plenty. The natural response is to tighten further, which extrudes the ring into the gap and produces a failure that looks like a material problem.

The fill limit also sets the tolerance on the groove depth. A groove machined 0.1 mm shallow on a 3 mm cord moves the fill by several percent, which is enough to take a comfortable design over the limit. That is why groove depth is a tighter tolerance than groove width on most drawings, even though it is the width that people dimension first.

Compression set is the clock

Compression set is measured by compressing a sample by a fixed percentage, holding it at temperature for a fixed time, releasing it and measuring how much it failed to recover. The number is a percentage of the original deflection, so 14 percent set means the ring came back to 86 percent of its original section.

For silicone the test conditions matter enormously. A ring that shows 12 percent set at 22 hours and 175 C can show 30 percent at 70 hours and 200 C. Quoting a set figure without the conditions is quoting nothing, and it is the most common gap in a silicone O-ring data sheet.

The practical consequence is that a silicone O-ring in a hot application should be sized for the set it will have at the end of life, not at the start. If the design needs 15 N to seal and the ring starts at 31 N with 14 percent set, there is room. If the application will take it to 30 percent set, the same ring ends near 22 N, and the margin is much thinner than the drawing suggested.

Squeeze Sealing force Compression set Where it is used
10 percent 12 N per 10 mm 8 percent Low pressure, easy assembly, vacuum
15 percent 21 N per 10 mm 11 percent Static seals, low temperature
20 percent 31 N per 10 mm 14 percent The general static seal compromise
25 percent 44 N per 10 mm 18 percent High pressure, or a worn groove
30 percent 60 N per 10 mm 24 percent Only where force matters more than life

Table 1 — Squeeze against force and set, and where each level is appropriate

Why silicone fails at temperature

Silicone's useful property is a wide service range, typically minus 60 to 200 C. Its weakness is that above about 150 C it continues to crosslink slowly in service, and the crosslinking makes it harder and less resilient. A ring that was 50 Shore A when it was fitted can be 60 Shore A after a year at 180 C, and a harder ring pushes back less at the same squeeze because it has taken a set.

The second mechanism is reversion, which is the opposite: at very high temperature and in a sealed environment, some silicone compounds depolymerise and go soft and tacky. Reversion is a compound problem rather than a design problem, and it is why a 200 C application needs a grade that is specified for 200 C continuous rather than one rated for 200 C peak.

Both mechanisms are accelerated by the presence of oil, which swells silicone more than most elastomers. A silicone O-ring in a mineral oil at 150 C will fail by swelling and softening long before it fails by heat alone, and that is a material selection error that no amount of groove design fixes.

Elastomer Continuous max Set at 175 C Mineral oil
Silicone, VMQ 200 C about 14 percent Poor, swells strongly
Fluorosilicone, FVMQ 200 C about 13 percent Buono
FKM 200 C about 12 percent Eccellente
EPDM 150 C about 15 percent Povero
NBR 100 C about 10 percent Buono
HNBR 150 C about 12 percent Buono

Table 2 — Why silicone is chosen, and the three cases where it should not be

What to specify

An O-ring specification that can be enforced names the application, not just the size.

  • Inside diameter, cord diameter and tolerance, on the actual standard used.
  • Hardness in Shore A, and whether a low-set grade is needed.
  • Compression set with the test conditions, since the bare percentage means nothing.
  • Squeeze percentage and groove fill, both stated on the drawing.
  • Service temperature, continuous and peak, and the fluid in contact.
  • Whether the ring is post-cured, which reduces outgassing in a sealed assembly.

Groove fill is the item to check first on any existing design. It is arithmetic, it takes a minute, and it explains a surprising number of joints that will not seal at any torque.

Myth: a thicker O-ring seals better because there is more rubber. A thicker ring in the same groove raises the fill, and past about 85 percent the joint cannot close. The seal depends on squeeze and on having somewhere for the displaced material to go, not on the amount of material.

What squeeze should a silicone O-ring have?

About 20 percent for a static seal. That gives roughly 31 N per 10 mm of circumference with a set of about 14 percent.

Why does more squeeze cause more compression set?

A more highly strained rubber relaxes more, so the permanent deformation left after release is larger. Squeeze buys force and costs life at the same time.

What is groove fill and why does it matter?

The ratio of the O-ring cross-section to the groove cross-section. Above about 85 percent there is no room for the displaced rubber and the joint will not close to metal-to-metal.

How do I compare compression set figures from two suppliers?

Only with the test conditions. 22 hours at 175 C and 70 hours at 200 C give very different numbers for the same compound.

Why do silicone O-rings harden in service?

Above about 150 C they continue to crosslink slowly, which raises hardness and reduces resilience, so the ring pushes back less at the same squeeze.

Can silicone O-rings be used in oil?

Only with care. Silicone swells strongly in mineral oil, and a swollen ring in a fixed groove over-fills it and leaks.

A joint that will not stop weeping?

Send the groove drawing, the pressure, the temperature and the fluid. We will check the fill and the squeeze, and tell you whether the ring or the groove is the problem.

Ask about silicone O-rings

Hi there! I'm John, dad and hero to awesome kid. By day, I'm a plastics manufacturing vet — injection molding, extrusion and vacuum forming — who went from factory floors to technical management. Here to share what I've learned—let's grow together!
it_ITIT

Chiedete un preventivo rapido

Inviare disegni e requisiti dettagliati via

Emial: [email protected]

Oppure compilate il modulo di contatto qui sotto: