Uplastech moulds precision thermoplastic components from 0.1 g micro parts to 2,000 g technical housings — with in-house mould making, engineering resins, and the first-article documentation your quality team will actually ask for.

0.1–2,000 gPart weight
±0.05 mmPrecision tolerance
Up to 40Cavities per tool

Up to 40-cavity precision tooling for high-volume programmes — with ±0.05 mm capability on critical features, in-house steel, and a parameter sheet that keeps shot 50,000 identical to shot one.

Injection Molding Product Types

Precision injection molded ABS housing, glass-filled nylon bracket and POM gear

Custom Injection Molding

General-purpose precision moulding for housings, covers, brackets and enclosures. Single and multi-cavity tools, engineering thermoplastics, cosmetic and functional finishes.

White POM and black PA66 precision gears being measured with a digital caliper

Precision Injection Molding

Tight-tolerance work held to ±0.05 mm: gears, connectors, sensor bodies and optical parts. Stable mould temperature control, SPC on critical dimensions, full dimensional reports.

Two-shot molded handle with rigid black ABS core and orange soft-touch TPE grip

Two-Shot Molding (2K)

Rigid and soft materials in one cycle. Soft-touch grips on tool bodies, colour-coded buttons, and TPE seals bonded directly to a structural substrate — no assembly, no adhesive.

Black molded knob with brass threaded inserts embedded in the base

Insert Molding

Brass, steel and threaded inserts moulded in place for load-bearing bosses. Stronger than heat-set inserts, and immune to pull-out and spin under torque.

Stack of thin-wall white polypropylene food containers with clear lids

Thin-Wall Injection Molding

Walls down to 0.6 mm for packaging, containers and lightweight enclosures. High-speed injection, fast-cycling tooling and precise flatness control on large panels.

Micro injection molded plastic parts beside a steel ruler and caliper

Micro Injection Molding

Sub-gram parts for medical devices, electronics and micro-fluidics. Micro-machined tooling, high injection velocity, and handling equipment that will not lose a 3 mg part.

Gas-assisted injection molded handle sectioned to show the hollow internal gas channel

Gas-Assisted Injection Molding

Hollow cores in thick sections without sink marks. Handles, levers and large panels gain stiffness with less material, shorter cycles and dramatically lower warpage.

Thick black structural foam molded panel with molded-in stiffening ribs

Structural Foam Molding

Thick-wall, large-footprint parts with a dense skin and cellular core. Low internal stress makes it the right answer for big housings that would warp if solid moulded.

Not sure which process fits your part? Send a STEP file — we will tell you which of the eight is cheapest to tool and run at your volume.

What Is Custom Injection Molding?

Thermoplastic pellets are dried, melted in a heated barrel, and forced under pressure into a closed steel cavity. The melt is held while it cools, then the part is ejected — finished, in one cycle, with no secondary shaping. Cycle times run from 8 seconds for a micro part to over 90 seconds for a thick technical component.

What separates a good moulder from an average one is not the machine. It is the tool, the drying discipline, and whether anyone is measuring the process instead of eyeballing the part. A 2 mm ABS housing that sinks, warps or flashes is almost never a machine problem — it is a tool or a parameter sheet problem, and both are decided before the first shot.

Injection Molding Capabilities

Capability Range
Part weight 0.1 g – 2,000 g
Maximum part size Approx. 600 × 400 × 250 mm
Cavitation 1 to 40 cavities
General tolerance ±0.10 mm (<100 mm), ±0.30 mm (100–300 mm)
Precision tolerance ±0.05 mm on critical features, with SPC
Wall thickness 0.6 mm – 6 mm
Mould steel P20 / 718H, NAK80, S136, H13
Mould life 100,000 – 1,000,000 shots by steel grade
Tooling lead time 25–45 days for a production tool
Surface finish SPI A1–D3, MT textures, high polish

Typical capability. Confirm the specific range against your drawing before quoting.

Engineering Resins We Mould

Bahan Penyusutan Drying Where it belongs
ABS 0.4–0.7% 80 °C / 2–3 h Housings, cosmetic covers, tool cases
PP 1.5–2.5% Not required Living hinges, caps, containers, trim
PC 0.5–0.7% 120 °C / 4 h Lenses, guards, electrical enclosures
PA6 / PA66 0.8–1.5% 80–100 °C / 4 h Gears, brackets, structural parts
POM 1.8–2.2% Not required Precision gears, clips, bearings
PBT / PET 0.3–0.8% 120 °C / 3–4 h Connectors, coil formers, electrical parts
PMMA 0.3–0.6% 80 °C / 3–4 h Light guides, display lenses, signage
PPSU / PSU 0.6–0.8% 150 °C / 4 h Sterilisable medical and food-service parts
TPE / TPU 1.0–2.0% 70–80 °C / 2 h Grips, seals, overmoulded soft-touch surfaces
PA-GF / PBT-GF 0.3–0.6% 100 °C / 4 h Structural parts needing stiffness and heat resistance

Indicative processing windows. Flame retardants, glass fillers and impact modifiers shift all three columns — always confirm against the grade datasheet.

How the Process Runs

  1. DFM review and mould design. We check wall thickness, draft, radii, undercuts and gate position against your drawing, and tell you which changes would cut your part price before steel is cut.
  2. Tool making. In-house CNC, EDM and wire cutting. Core and cavity steel is selected against your volume, not against the cheapest quote.
  3. T1 sampling. First shots are measured against a ballooned drawing and reported, not just photographed.
  4. Parameter freeze. Mould temperature, packing profile and cooling time are locked into a set-up sheet so shot 50,000 matches shot 1.
  5. Production and SPC. Critical dimensions are checked on a defined frequency; out-of-trend data triggers a process adjustment, not a rework loop.
  6. Finishing and packing. Degating, ultrasonic welding, pad printing, assembly and clean-room packing as specified.

Aplikasi

  • Otomotif — interior trim clips, sensor housings, under-hood brackets in PA-GF, fluid reservoirs.
  • Medical and laboratory — instrument housings, fluidic cartridges, sterilisable trays in PPSU.
  • Elektronik — connector bodies, coil formers, enclosures with EMI-shielding options.
  • Industrial equipment — machine guards, cable management, pneumatic fittings.
  • Consumer and appliance — cosmetic housings, two-shot handles, thin-wall packaging.

Kontrol Kualitas

Every production run ships with a first-article inspection report, a dimensional report against the agreed critical characteristics, and material certificates traceable to the resin batch. Where the part carries a cosmetic requirement, we agree the A-surface and a limit sample before T1 — because "looks fine" is not a specification, and arguing about it after 20,000 parts is expensive for both sides.

Send us a STEP file and your annual volume. You will get a manufacturability review, a tooling recommendation, and an indicative part price — including an honest note if a different process would be cheaper for your geometry.

Frequently Asked Questions

What is the minimum order quantity for custom injection molding?

There is no technical minimum — we will run 200 pieces if the tooling is justified. The economic threshold is usually 1,000–2,000 pieces, below which vacuum forming or CNC machining is cheaper once tooling is amortised.

How much does an injection mold cost?

A single-cavity P20 production tool for a part under 150 mm typically runs $4,000–$12,000. Medium housings with side actions run $12,000–$30,000, and large multi-cavity tools $30,000–$90,000. Steel grade, cavitation, hot runner and polish level are the four biggest levers.

How long does it take from design to delivery?

Usually 5–8 weeks: 3–7 days for DFM and mould design sign-off, 25–45 days for tool making, then T1 sampling and any correction, then production. Tools with multiple slides add two to three weeks.

Can you mould parts from our existing tool?

Yes. We start with a mould condition inspection and a dimensional report before the first production run, so any pre-existing wear is documented and agreed before it becomes a dispute.

Do you offer overmolding and two-shot parts?

Yes — rigid substrate with TPE or TPU overmould, either in a two-shot tool or as a sequential overmould on a pre-moulded insert. Material pairing matters: not every TPE bonds to every substrate, and we will confirm adhesion before committing to a tool.

What documentation comes with a shipment?

First-article inspection report, dimensional report on agreed critical characteristics, material certificate with batch traceability, and a process parameter sheet on request. PPAP-style documentation is available for automotive programmes.

Get a DFM review before you commit to tooling

Upload your part and target volume. We return a manufacturability review, tooling cost, cycle time estimate and an indicative part price.

Request a quote

id_IDID

Minta Penawaran Cepat

Kirim gambar dan persyaratan terperinci melalui

Emial: [email protected]

Atau Isi Formulir Kontak di bawah ini: