FVMQ exists to solve a specific conflict: silicone is superb in the cold but swells in fuel, and fluorocarbon resists fuel but stiffens in the cold. Fluorosilicone sits between them — flexible to -60 °C while resisting jet fuel, diesel and aromatic solvents. It is the material of choice for aerospace fuel systems and automotive fuel-handling seals, and it is priced accordingly.

Custom FVMQ Fluorosilicone Rubber Moulding — Aircraft fuel system seals and gaskets

50 – 80 Shore AHardness range
-60 to +200 °CService temperature
7 – 10 MPaTensile strength

Typical values for standard moulding grades. Exact figures depend on the specific compound or grade — confirm against your drawing before quoting.

Key properties

الممتلكات Typical value
Hardness range 50 – 80 Shore A
Service temperature -60 to +200 °C
Tensile strength 7 – 10 MPa
Elongation at break 150 – 400 %
Compression set (22 h / 175 °C) 20 – 35 %
Fuel resistance Good — low swell in jet and diesel fuel

Values are typical for unfilled moulding grades at 23 °C unless stated. Glass-filled and specialty grades differ.

Typical applications

  • Aircraft fuel system seals and gaskets
  • Automotive fuel pump and injector seals
  • Diaphragms in fuel-handling equipment
  • Seals exposed to aromatic solvents
  • Cryogenic and low-temperature sealing

Processing notes

  • FVMQ swells less than VMQ in fuel but still swells measurably. Design gland volume with the swell allowance, not against it.
  • Tear strength is lower than fluorocarbon. Avoid sharp sealing edges and specify generous radii.
  • Cost is several times that of silicone. Use it only where the low-temperature plus fuel combination is genuinely required — otherwise FKM or VMQ will do the job for less.
  • Bonding to metal needs a fluorosilicone-specific primer; standard silicone primers do not hold.
Tooling, not just material. Every material above behaves differently in the tool — shrinkage, gate position, cooling and ejection all change. We review the DFM against the specific grade before the tool is cut, so the first shot is a sample, not a surprise.

Frequently asked questions

FVMQ or FKM for a fuel seal?

FKM if the lowest service temperature is above about -20 °C — it resists fuel better and costs less. FVMQ when the seal must stay flexible below -40 °C, which is where FKM stiffens and leaks.

Is FVMQ suitable for aviation use?

Yes, in grades meeting the relevant aerospace specifications. Tell us the spec number and we will confirm the compound and the test documentation before quoting.

Related materials

← All Rubber & Silicone Solutions

Send us your FVMQ Fluorosilicone Rubber drawing

Upload a 3D model or a 2D drawing and we will come back with a DFM review, a tooling cost and a piece price — usually within two working days.

Request a quote

arAR

اطلب عرض أسعار سريع

إرسال الرسومات والمتطلبات التفصيلية عبر

إميال: [email protected]

أو املأ نموذج الاتصال أدناه: