Polycarbonate is what you specify when a part has to be transparent and survive being hit. It carries roughly 200 times the impact energy of glass at a fraction of the weight, holds clarity up to 120 °C, and takes a flame-retardant grade without turning opaque. The trade-off is that it is fussy about moisture and needs a hot mould — both of which are process disciplines, not material limits.

Custom PC Injection Molding — Machine guards and transparent covers

125 – 135 °CHDT at 1.8 MPa
60 – 70 MPaTensile strength
1.20 g/cm³Yoğunluk

Typical values for standard moulding grades. Exact figures depend on the specific compound or grade — confirm against your drawing before quoting.

Key properties

Mülkiyet Typical value
Yoğunluk 1.20 g/cm³
Tensile strength 60 – 70 MPa
Flexural modulus 2.3 – 2.4 GPa
HDT at 1.8 MPa 125 – 135 °C
Mould shrinkage 0.5 – 0.7 %
Light transmission 88 – 90 % at 3 mm

Values are typical for unfilled moulding grades at 23 °C unless stated. Glass-filled and specialty grades differ.

Typical applications

  • Machine guards and transparent covers
  • LED light diffusers and lenses
  • Medical device housings and fluid paths
  • Safety helmets and protective visors
  • Electrical enclosures requiring flame retardancy

Processing notes

  • Dry 4 h at 120 °C. This is not optional — 0.02 % residual moisture is enough to hydrolyse the melt and drop impact strength by half.
  • Melt 280 – 310 °C, mould 80 – 110 °C. A cold mould locks in stress and produces parts that craze weeks later.
  • Annealing at 110 – 120 °C for 1 – 2 h relieves moulded-in stress where the part will meet solvents or sustained load.
  • Gate away from high-stress zones and avoid sharp internal corners; PC notches rather than yields.
Tooling, not just material. Every material above behaves differently in the tool — shrinkage, gate position, cooling and ejection all change. We review the DFM against the specific grade before the tool is cut, so the first shot is a sample, not a surprise.

Frequently asked questions

Will the part stay clear after years outdoors?

Standard PC yellows under UV. For outdoor clarity we specify a UV-coated grade or add a hard-coat after moulding. If the part is purely structural, an opaque PC/ABS blend is cheaper and tougher at the edges.

Can PC be overmoulded with a soft-touch material?

Yes, with a TPE or TPU grade formulated for PC adhesion. The PC insert needs to be dry and the bond improves markedly if the insert is preheated to around 80 °C.

Related materials

← All Injection Molding Solutions

Send us your PC drawing

Upload a 3D model or a 2D drawing and we will come back with a DFM review, a tooling cost and a piece price — usually within two working days.