The problem
Symptom. A customer releases a profile on its metre-weight capability, but metre weight hides a local thin wall that fails the dimension on a downstream fit.
What it costs. A fit failure at the customer forces an illustrative 11 h of investigation and a stop-ship while the wall is measured separately.
This article separates metre-weight capability from wall-thickness capability, sets the wall check, and writes both into the control plan.
When metre weight hides a thin wall
In one illustrative case a profile shows a strong metre-weight capability of about 1.5, so the customer releases it, but a local wall thin spot drops the wall capability to 0.7 and the part fails the fit.
| Capability trigger | What it hides | First figure to check |
|---|---|---|
| Weight used as proxy | Wall not seen | Wall CpK vs 1.33 |
| Fit fails downstream | Stop-ship raised | Illustrative 11 h probe |
| Weight looks safe | Release mistaken | Local thin spot |
| Tool not adjusted | Recurs next lot | Wall measured |
Table 1 - Reading a metre-weight proxy before measuring the wall
Need a fixed price for this profile?
Send the cross-section drawing, material, cut length and annual volume. We will review die, calibration and tolerance, then return a written tooling and production quotation.
Quantify the wall versus metre-weight capability
Separate the two before trusting them. Five sample groups return illustrative wall capability indices of 1.1, 0.9, 0.7, 1.0 and 1.2 against a metre-weight capability held near 1.5; the wall dips below the 1.33 line while weight stays safe. These are illustrative worked values from stated assumptions, not a measured series or a quoted result.
A five-step diagnostic sequence
- Weigh the profile.
Confirm the metre-weight capability is within its stated band. - Section the wall.
Cut a cross-section and measure the local wall thickness. - Find the thin spot.
Flag any wall capability below the 1.33 line. - Adjust the tool.
Change the die so the wall clears the limit, then re-measure. - File the plan.
Record both capabilities so the next lot uses the same checks.
The chart below is a typical result from that measurement step. Use it to separate a design limit from a setting that can still be recovered.

Set the wall-thickness check alongside weight
Set the check at both weight and wall. With the wall measured on its own, the 0.7 capability is caught and the tool adjusted; an illustrative 11 h of investigation is the cost of releasing on weight alone. These are illustrative worked values from stated assumptions, not a market survey, a quoted price or a measured series.
| Clause or parameter | Agreed value | What goes wrong outside it |
|---|---|---|
| Metre-weight CpK | Monitored per lot | Proxy for wall |
| Wall CpK | Separate check | Thin spot missed |
| Wall limit | 1.33 stated | Fit fails |
| Plan owner | Named per programme | Capability applied loosely |
Table 2 - Capability clauses for the control plan
A controlled measurement sequence
Run the measurement in a fixed order: weigh, section the wall, measure the thin spot, then compare. The table ranks the actions by fit risk so the wall is never proxied by weight.
| Control action | What it fixes | Cost or trade-off |
|---|---|---|
| Measure the wall | Thin spot caught | Section to cut |
| Keep weight check | Trend monitored | Scale to maintain |
| State both limits | No proxy | Plan longer |
| Re-check on change | No drift after change | One owner to maintain |
Table 3 - Capability controls ranked by fit risk
Write both capabilities into the control plan
Put both in the control plan: a metre-weight capability and a separate wall-thickness capability, each with its own limit. A written plan turns a proxy release into a verified fit.
Need the section checked before tooling?
Send us the section and the installation conditions. We will review wall balance, tolerance and fixing detail, then return a marked-up drawing with a tooling quotation.
What to send us
- Cross-section drawing with wall thicknesses
- Material and colour
- Installation temperature range
- Fixing method and run length
Keep the checks current between changes
Re-check both at each change, record the 11 h actually avoided, and re-forecast the capability needs. A written plan reviewed on dated evidence settles the capability question at release rather than at the customer.
Before you release this extruded profile
- The control plan measures wall thickness capability separately from metre weight
- A local thin spot is flagged when wall CpK falls below 1.33
- Metre weight is not used as the sole release proxy
- Both capabilities are re-checked at each process change
- A named owner maintains the capability checks
Write the measurement temperature and the tolerance into the drawing; most disputes are really about how the part was measured.
Why not release on weight?
Metre weight averages the whole section, so a local thin wall is hidden. The part can pass on weight and still fail the fit.
How much does the proxy cost?
Using illustrative assumptions the fit failure and stop-ship cost 11 h of investigation. These are worked example values, not a measured series.
What limit applies to the wall?
A stated 1.33 capability. In this illustrative case the wall dips to 0.7 while weight stays near 1.5.
Can weight stay as a check?
Yes, as a trend monitor, but never as the only release gate. The wall needs its own measurement.
Who owns the checks?
A named programme owner re-checks both at changes. Without one owner the wall is proxied again.
Do the checks expire?
They are valid until the process changes. Re-checking at each change keeps the capability evidence current.
Get a profile that holds its dimension
Send us the profile section, the length and the service conditions. We will review die, calibration and tolerance, then quote tooling and production with a defined measurement method.
To get an accurate quote, send:
- Profile cross-section drawing
- Material and colour
- Cut length and annual volume
- Service temperature and exposure
Prefer to talk it through first?
Электронная почта [email protected] or message us on WhatsApp +86 177 1752 9949. Send a drawing, a sample or a specification and an engineer will reply.
Why buyers work with Uplastech
ISO 9001, ISO 14001 and ISO 45001 certified. Founded in 2016, with injection moulding lines in Shanghai and an extrusion plant in Jiangsu. Moulding machines from 90T to 1100T and a maximum shot weight of 5100 g. Samples and a written quotation are available on request.
Continue reading
- Extrusion dimensional drift
- Extrusion profile tolerance
- Profile calibration and cooling
- PVC profile weathering and colour
- PVC window profile design
Ready to specify? See our plastic profile extrusion services или request a written quotation.