{"id":9738,"date":"2024-02-15T01:00:00","date_gmt":"2024-02-15T01:00:00","guid":{"rendered":"https:\/\/uplastech.com\/profile-cut-length-gauge-calibration-tolerance\/"},"modified":"2026-11-08T08:18:46","modified_gmt":"2026-11-08T08:18:46","slug":"profile-cut-length-gauge-calibration-tolerance","status":"publish","type":"post","link":"https:\/\/uplastech.com\/ru\/profile-cut-length-gauge-calibration-tolerance\/","title":{"rendered":"Cut-Length Gauge Calibration and Tolerance Band"},"content":{"rendered":"<style>\n.upl-blog{font-size:17px;line-height:1.78;color:#1f2937}\n.upl-blog p{margin:0 0 18px}\n.upl-blog h2{font-size:26px;line-height:1.3;color:#0b2b33;margin:46px 0 14px;font-weight:700;letter-spacing:-.015em}\n.upl-blog h3{font-size:19.5px;color:#0d3b47;margin:28px 0 10px;font-weight:700}\n.upl-blog ul,.upl-blog ol{margin:0 0 20px;padding-left:22px}\n.upl-blog li{margin:0 0 9px}\n.upl-blog figure{margin:0 0 34px}\n.upl-blog figure img{width:100%;height:auto;display:block;border-radius:10px}\n.upl-blog figcaption{font-size:13px;color:#6b7280;margin-top:10px;line-height:1.5}\n.upl-blog .toc{background:none;border:0;border-radius:0;padding:0;margin:0 0 34px}\n.upl-blog .toc .lwptoc{margin:0}\n.upl-blog .toc h4{margin:0 0 10px;font-size:13px;letter-spacing:.1em;text-transform:uppercase;color:#0d5563}\n.upl-blog .toc ol{margin:0;padding-left:18px;font-size:14.5px}\n.upl-blog .toc li{margin-bottom:6px}\n.upl-blog table{width:100%;border-collapse:collapse;font-size:14.5px;margin:0 0 10px}\n.upl-blog th{background:#0d3b47;color:#fff;text-align:left;padding:11px 13px;font-weight:600;font-size:13.5px;border:0}\n.upl-blog td{padding:11px 13px;border:0;border-bottom:1px solid #e8ebed;vertical-align:top}\n.upl-blog tbody tr:nth-child(even){background:#fafbfc}\n.upl-blog .tablecap{font-size:12.5px;color:#6b7280;margin:0 0 30px}\n.upl-blog .myth{background:#fff8ef;border:1px solid #f6ddbd;border-radius:8px;padding:16px 20px;margin:0 0 26px;font-size:15.5px}\n.upl-blog .myth b{color:#a85c10}\n.upl-blog .callout{background:#f2f8f9;border-radius:8px;padding:18px 22px;margin:0 0 26px;font-size:15.5px;border-left:3px solid #14707f}\n.upl-blog .faq h3{border-top:1px solid #eceff1;padding-top:22px;margin-top:0;font-size:18px}\n.upl-blog .faq h3:first-of-type{border-top:0;padding-top:0}\n.upl-blog .cta{background:linear-gradient(135deg,#0b2b33,#0d5563);color:#fff;border-radius:12px;padding:34px;margin:48px 0 30px}\n.upl-blog .cta h2,.upl-blog .cta .cta-h{color:#fff;margin:0 0 10px;font-size:24px;font-weight:700;line-height:1.3}\n.upl-blog .cta p{color:#c9dee3;margin:0 0 20px;font-size:16px}\n.upl-blog .btn{display:inline-block;background:#e07a1f;color:#fff;text-decoration:none;font-weight:700;padding:13px 26px;border-radius:8px;font-size:15.5px}\n.upl-blog .rel{border-top:1px solid #e8ebed;margin-top:40px;padding-top:26px}\n.upl-blog .rel h4{font-size:13px;letter-spacing:.1em;text-transform:uppercase;color:#6b7280;margin:0 0 14px}\n.upl-blog .rel ul{list-style:none;padding:0;margin:0}\n.upl-blog .rel li{padding:11px 0;border-bottom:1px dashed #e8ebed}\n.upl-blog .rel a{text-decoration:none;font-weight:600;font-size:15.5px}\n\/* ==UPL-CONVERSION-MODULES-START== 2024 problem-solving \/ lead-gen blocks *\/\n.upl-blog .mod-h{font-size:12.5px;letter-spacing:.12em;text-transform:uppercase;font-weight:700;color:#0d5563;margin:0 0 12px}\n.upl-blog .problem{background:#fff8f3;border:1px solid #f3ddc9;border-left:4px solid #e07a1f;border-radius:10px;padding:22px 26px;margin:0 0 32px;font-size:16px}\n.upl-blog .problem p{margin:0 0 10px}\n.upl-blog .problem p:last-child{margin-bottom:0}\n.upl-blog .problem .mod-h{color:#a85c10}\n.upl-blog .problem .problem-promise{font-weight:700;color:#0b2b33}\n.upl-blog .steps{background:#f7fafb;border:1px solid #e1ebee;border-radius:10px;padding:22px 26px;margin:0 0 28px}\n.upl-blog .steps ol{list-style:none;counter-reset:uplst;margin:0;padding:0}\n.upl-blog .steps li{counter-increment:uplst;position:relative;padding:0 0 16px 42px;margin:0;font-size:15.5px}\n.upl-blog .steps li:last-child{padding-bottom:0}\n.upl-blog .steps li::before{content:counter(uplst);position:absolute;left:0;top:2px;width:26px;height:26px;border-radius:50%;background:#0d5563;color:#fff;font-size:13px;font-weight:700;line-height:26px;text-align:center}\n.upl-blog table.spec th{background:#14707f}\n.upl-blog .conv{background:#eef6f7;border:1px solid #cfe4e8;border-radius:10px;padding:24px 26px;margin:32px 0}\n.upl-blog .conv p{margin:0 0 12px;font-size:15.5px}\n.upl-blog .conv .conv-lbl{font-weight:700;color:#0b2b33;margin:16px 0 8px}\n.upl-blog ul.conv-need{list-style:none;padding:0;margin:0 0 20px;display:grid;grid-template-columns:1fr 1fr;gap:6px 18px}\n.upl-blog ul.conv-need li{position:relative;padding-left:20px;margin:0;font-size:14.5px}\n.upl-blog ul.conv-need li::before{content:\"\";position:absolute;left:0;top:9px;width:9px;height:9px;border:2px solid #14707f;border-radius:2px}\n.upl-blog .conv-btn{display:inline-block;background:#0d5563;color:#fff;text-decoration:none;font-weight:700;padding:11px 22px;border-radius:7px;font-size:15px}\n.upl-blog .checklist{background:#fbfcfd;border:1px solid #e3e9ec;border-radius:10px;padding:24px 26px;margin:36px 0}\n.upl-blog .checklist ul{list-style:none;padding:0;margin:0 0 12px}\n.upl-blog .checklist li{position:relative;padding-left:28px;margin:0 0 10px;font-size:15.5px}\n.upl-blog .checklist li::before{content:\"\";position:absolute;left:0;top:7px;width:14px;height:14px;border:2px solid #0d5563;border-radius:3px}\n.upl-blog .cl-note{font-size:13.5px;color:#6b7280;margin:0}\n.upl-blog .cta .cta-lbl{color:#c9dee3;font-weight:700;margin:0 0 8px;font-size:14.5px}\n.upl-blog ul.cta-need{list-style:none;padding:0;margin:0 0 22px;display:grid;grid-template-columns:1fr 1fr;gap:4px 18px}\n.upl-blog ul.cta-need li{color:#e4f0f2;font-size:14.5px;padding-left:18px;position:relative;margin:0}\n.upl-blog ul.cta-need li::before{content:\"\\2713\";position:absolute;left:0;color:#e07a1f;font-weight:700}\n\/* ==UPL-CONVERSION-MODULES-END== *\/\n@media(max-width:640px){.upl-blog h2{font-size:22px}.upl-blog table{font-size:13px}.upl-blog .cta{padding:24px}.upl-blog ul.conv-need,.upl-blog ul.cta-need{grid-template-columns:1fr}.upl-blog .problem,.upl-blog .steps,.upl-blog .conv,.upl-blog .checklist{padding:18px}}\n\/* \u5355\u7bc7\u9875\u9690\u85cf WhatsApp \u95ee\u5019\u5361\uff0c\u53ea\u4fdd\u7559\u5706\u5f62\u6c14\u6ce1\uff0c\u907f\u514d\u906e\u6321\u4fa7\u680f\u8be2\u76d8\u63d0\u4ea4\u6309\u94ae\u3002\n   \u6ce8\u610f\uff1aClick to Chat \u7684\u70b9\u51fb\u903b\u8f91\u662f\u300c\u95ee\u5019\u5361\u5143\u7d20\u5b58\u5728\u5c31\u4e0d\u8df3\u8f6c\u300d\uff0c\u53ea\u9760 CSS \u9690\u85cf\u4f1a\u8ba9\u6c14\u6ce1\u53d8\u6210\u6b7b\u94fe\u63a5\u3002\n   Code Snippets #9\u300cUPL single post: WhatsApp bubble jumps straight to chat\u300d\u8d1f\u8d23\u628a\u8be5\u8282\u70b9\u4ece DOM \u79fb\u9664\uff0c\n   \u4e0b\u9762\u8fd9\u6761 CSS \u53ea\u662f\u79fb\u9664\u524d\u7684\u89c6\u89c9\u515c\u5e95\u3002\u5220 #9 \u524d\u5fc5\u987b\u5148\u5220\u8fd9\u6761\u89c4\u5219\u3002 *\/\nbody.single-post .ht_ctc_chat_greetings_box{display:none !important}\n<\/style>\n<div class=\"upl-blog\">\n<figure>\n<img fetchpriority=\"high\" decoding=\"async\" src=\"https:\/\/uplastech.com\/wp-content\/uploads\/2026\/11\/2024-profile-cut-length-gauge-calibration-tolerance-hero-scaled.jpg\" alt=\"Real extruded plastic profiles and pipe on a production site\" width=\"1536\" height=\"909\"><figcaption>Real plastic profile extrusion production context. Photo: Pexels.<\/figcaption><\/figure>\n<div class=\"problem\">\n<p class=\"mod-h\">The problem<\/p>\n<p><b>Symptom.<\/b> A cut-length gauge drifts out of calibration and the tolerance band is shared unevenly, so cut bars come back long at one end of the run and short at the other.<\/p>\n<p><b>What it costs.<\/b> Sorting and re-cutting the out-of-band stock costs an illustrative 9 h and a hold while the gauge is calibrated and the band is allocated.<\/p>\n<p class=\"problem-promise\">This article quantifies the length error by gauge check, sets the calibration and band, and writes the rule into the cut plan.<\/p>\n<\/div>\n<div class=\"toc\"><\/div>\n<h2 id=\"when-cut-length-drifts-with-the-gauge\">When cut length drifts with the gauge<\/h2>\n<p>In one illustrative case a cut-length gauge drifts out of calibration and the tolerance band is shared so the bar can sit at either edge, so cut lengths return errors up to 1.3 mm against a 1.0 mm tolerance.<\/p>\n<table>\n<thead>\n<tr>\n<th>Gauge trigger<\/th>\n<th>What it causes<\/th>\n<th>First figure to check<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>Gauge drift<\/td>\n<td>Length error<\/td>\n<td>Error vs 1.0 mm<\/td>\n<\/tr>\n<tr>\n<td>Band shared<\/td>\n<td>Bar at either edge<\/td>\n<td>Illustrative 9 h recut<\/td>\n<\/tr>\n<tr>\n<td>Out-of-band stock<\/td>\n<td>Hold raised<\/td>\n<td>Calibration date<\/td>\n<\/tr>\n<tr>\n<td>Customer rejects<\/td>\n<td>Length disputed<\/td>\n<td>Band allocated<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p class=\"tablecap\">Table 1 - Reading a cut-length gauge drift before re-calibrating<\/p>\n<div class=\"callout\">Record which of these you are actually seeing before changing any setting. Two faults can look identical on the line and need opposite corrections.<\/div>\n<p><!-- upl-conv-v1 quickcta --><\/p>\n<div class=\"quickcta\">\n<p class=\"mod-h\">Need a fixed price for this profile?<\/p>\n<p>Send the cross-section drawing, material, cut length and annual volume. We will review die, calibration and tolerance, then return a written tooling and production quotation.<\/p>\n<p class=\"quickcta-act\"><a class=\"quickcta-btn\" href=\"https:\/\/uplastech.com\/plastic-extrusion-solutions\/\">Get a profile quotation<\/a><a class=\"quickcta-alt\" href=\"mailto:john@uplastech.com\">Email john@uplastech.com<\/a><a class=\"quickcta-alt\" href=\"https:\/\/wa.me\/8617717529949\">WhatsApp<\/a><\/p>\n<\/div>\n<h2 id=\"quantify-the-length-error-by-gauge-check\">Quantify the length error by gauge check<\/h2>\n<p>Quantify the error before correcting it. Five gauge checks return illustrative length errors of 0.4, 0.8, 1.3, 1.0 and 0.6 mm; the worst crosses the 1.0 mm tolerance because the band is not allocated. These are illustrative worked values from stated assumptions, not a measured series or a quoted result.<\/p>\n<div class=\"steps\">\n<p class=\"mod-h\">A five-step diagnostic sequence<\/p>\n<ol>\n<li><b>Calibrate the gauge.<\/b><br \/>Confirm the cut-length gauge is within calibration before any cut.<\/li>\n<li><b>Allocate the band.<\/b><br \/>Centre the tolerance band so the bar cannot sit at either edge.<\/li>\n<li><b>Set the cut.<\/b><br \/>Apply the calibrated gauge and the centred band to the cut length.<\/li>\n<li><b>Verify the length.<\/b><br \/>Measure a cut bar to confirm the error is under 1.0 mm.<\/li>\n<li><b>File the plan.<\/b><br \/>Record the calibration date and band so the next cut uses the same rule.<\/li>\n<\/ol>\n<\/div>\n<p>The chart below is a typical result from that measurement step. Use it to separate a design limit from a setting that can still be recovered.<\/p>\n<figure>\n<img decoding=\"async\" src=\"https:\/\/uplastech.com\/wp-content\/uploads\/2026\/11\/profile-cut-length-gauge-calibration-tolerance-chart.jpg\" alt=\"Cut-Length Gauge Calibration and Tolerance Band: calculated response trend and an illustrative root-cause split\" width=\"1536\" height=\"909\"><figcaption>Figure 1 \u2014 Calculated response trend and an illustrative root-cause split. Values are engineering guidance for diagnosis, not a measured survey; confirm them on your own line before changing a drawing or a specification.<\/figcaption><\/figure>\n<h2 id=\"set-the-calibration-and-tolerance-band\">Set the calibration and tolerance band<\/h2>\n<p>Set the rule at a calibrated gauge and a centred tolerance band. With the gauge calibrated and the band allocated, the error stays under 1.0 mm; an illustrative 9 h of re-cut is the cost of the drift. These are illustrative worked values from stated assumptions, not a market survey, a quoted price or a measured series.<\/p>\n<table class=\"spec\">\n<thead>\n<tr>\n<th>Clause or parameter<\/th>\n<th>Agreed value<\/th>\n<th>What goes wrong outside it<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>Gauge calibration<\/td>\n<td>Within date<\/td>\n<td>Length error<\/td>\n<\/tr>\n<tr>\n<td>Tolerance band<\/td>\n<td>Centred per cut<\/td>\n<td>Bar at edge<\/td>\n<\/tr>\n<tr>\n<td>Re-cal interval<\/td>\n<td>Stated per gauge<\/td>\n<td>Drift surprise<\/td>\n<\/tr>\n<tr>\n<td>Plan owner<\/td>\n<td>Named per programme<\/td>\n<td>Rule applied loosely<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p class=\"tablecap\">Table 2 - Cut-length clauses for the cut plan<\/p>\n<h2 id=\"a-controlled-gauge-and-cut-sequence\">A controlled gauge-and-cut sequence<\/h2>\n<p>Run the sequence in a fixed order: calibrate, allocate the band, set the cut, then verify. The table ranks the actions by escape risk so the gauge is never the hidden variable.<\/p>\n<table>\n<thead>\n<tr>\n<th>Control action<\/th>\n<th>What it fixes<\/th>\n<th>Cost or trade-off<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>Calibrate the gauge<\/td>\n<td>Error controlled<\/td>\n<td>Calibration time<\/td>\n<\/tr>\n<tr>\n<td>Centre the band<\/td>\n<td>No edge drift<\/td>\n<td>Band to allocate<\/td>\n<\/tr>\n<tr>\n<td>Re-cal on date<\/td>\n<td>No surprise drift<\/td>\n<td>Schedule to keep<\/td>\n<\/tr>\n<tr>\n<td>Review on change<\/td>\n<td>No drift after change<\/td>\n<td>One owner to maintain<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p class=\"tablecap\">Table 3 - Cut-length controls ranked by escape risk<\/p>\n<div class=\"myth\"><b>Myth:<\/b> \"A process adjustment will fix it.\" Once a design limit is reached, more tuning only adds cost and variation. Confirm the limit with a measurement, then change the drawing or the specification.<\/div>\n<h2 id=\"write-the-calibration-rule-into-the-cut-plan\">Write the calibration rule into the cut plan<\/h2>\n<p>Put the rule in the cut plan: a calibrated gauge, a centred tolerance band, and a re-calibration date. A written rule turns a drifting cut into a controlled length.<\/p>\n<div class=\"conv\">\n<p class=\"mod-h\">Need the section checked before tooling?<\/p>\n<p>Send us the section and the installation conditions. We will review wall balance, tolerance and fixing detail, then return a marked-up drawing with a tooling quotation.<\/p>\n<p class=\"conv-lbl\">What to send us<\/p>\n<ul class=\"conv-need\">\n<li>Cross-section drawing with wall thicknesses<\/li>\n<li>Material and colour<\/li>\n<li>Installation temperature range<\/li>\n<li>Fixing method and run length<\/li>\n<\/ul>\n<p><a class=\"conv-btn\" href=\"\/plastic-extrusion-solutions\/\">Send the section drawing<\/a>\n<\/div>\n<h2 id=\"keep-the-gauge-current-between-calibrations\">Keep the gauge current between calibrations<\/h2>\n<p>Re-calibrate at each interval, record the 9 h actually avoided, and re-forecast the gauge needs. A written plan reviewed on dated evidence settles the length question at cut rather than at the customer.<\/p>\n<div class=\"callout\">Validate one change at a time and keep the measurement record. A supplier discussion backed by data is resolved in days, not weeks.<\/div>\n<div class=\"checklist\">\n<p class=\"mod-h\">Before you release this extruded profile<\/p>\n<ul>\n<li>The cut plan uses a cut-length gauge within calibration<\/li>\n<li>The tolerance band is centred, not shared to either edge<\/li>\n<li>A re-calibration date is scheduled and kept<\/li>\n<li>Cut length is verified against the 1.0 mm tolerance<\/li>\n<li>A named owner maintains the gauge between calibrations<\/li>\n<\/ul>\n<p class=\"cl-note\">Write the measurement temperature and the tolerance into the drawing; most disputes are really about how the part was measured.<\/p>\n<\/div>\n<div class=\"faq\">\n<h3>Why calibrate the cut gauge?<\/h3>\n<p>A drifting gauge pushes cut lengths to the tolerance edge, so bars come back long at one end and short at the other. Calibration keeps the error centred.<\/p>\n<h3>How much does the drift cost?<\/h3>\n<p>Using illustrative assumptions sorting and re-cutting costs 9 h and a hold. These are worked example values, not a measured series.<\/p>\n<h3>What tolerance applies?<\/h3>\n<p>A stated 1.0 mm cut-length tolerance. In this illustrative case the worst check reads 1.3 mm, over the line.<\/p>\n<h3>Why centre the band?<\/h3>\n<p>A shared band lets the bar sit at either edge; centring it removes the edge drift that causes the dispute.<\/p>\n<h3>Who owns the gauge?<\/h3>\n<p>A named programme owner re-calibrates on schedule. Without one owner the date is missed.<\/p>\n<h3>Does the rule expire?<\/h3>\n<p>It is valid until the re-calibration date. Keeping the schedule current keeps the cut evidence current.<\/p>\n<\/div>\n<div class=\"cta\">\n<p class=\"cta-h\">Get a profile that holds its dimension<\/p>\n<p>Send us the profile section, the length and the service conditions. We will review die, calibration and tolerance, then quote tooling and production with a defined measurement method.<\/p>\n<p class=\"cta-lbl\">To get an accurate quote, send:<\/p>\n<ul class=\"cta-need\">\n<li>Profile cross-section drawing<\/li>\n<li>Material and colour<\/li>\n<li>Cut length and annual volume<\/li>\n<li>Service temperature and exposure<\/li>\n<\/ul>\n<p><a class=\"btn\" href=\"\/plastic-extrusion-solutions\/\">Request a profile quotation<\/a><br \/>\n<!-- upl-conv-v1 contact --><\/p>\n<div class=\"contactbar\">\n<p class=\"contactbar-h\">Prefer to talk it through first?<\/p>\n<p>Email <a href=\"mailto:john@uplastech.com\">john@uplastech.com<\/a> or message us on <a href=\"https:\/\/wa.me\/8617717529949\">WhatsApp +86 177 1752 9949<\/a>. Send a drawing, a sample or a specification and an engineer will reply.<\/p>\n<\/div>\n<p><!-- upl-conv-v1 trust --><\/p>\n<div class=\"trust\">\n<p class=\"trust-h\">Why buyers work with Uplastech<\/p>\n<p>ISO 9001, ISO 14001 and ISO 45001 certified. Founded in 2016, with injection moulding lines in Shanghai and an extrusion plant in Jiangsu. Moulding machines from 90T to 1100T and a maximum shot weight of 5100 g. Samples and a written quotation are available on request.<\/p>\n<\/div>\n<\/div>\n<div class=\"rel\">\n<h4>Continue reading<\/h4>\n<ul>\n<li><a href=\"https:\/\/uplastech.com\/extrusion-dimensional-drift\/\">Extrusion dimensional drift<\/a><\/li>\n<li><a href=\"https:\/\/uplastech.com\/extrusion-profile-tolerance\/\">Extrusion profile tolerance<\/a><\/li>\n<li><a href=\"https:\/\/uplastech.com\/profile-calibration-cooling\/\">Profile calibration and cooling<\/a><\/li>\n<li><a href=\"https:\/\/uplastech.com\/pvc-profile-weathering-colour\/\">PVC profile weathering and colour<\/a><\/li>\n<li><a href=\"https:\/\/uplastech.com\/pvc-window-profile-design\/\">PVC window profile design<\/a><\/li>\n<\/ul>\n<p><!-- upl-conv-v1 service --><\/p>\n<p class=\"rel-svc\">Ready to specify? See our <a href=\"https:\/\/uplastech.com\/plastic-extrusion-solutions\/\">plastic profile extrusion services<\/a> or <a href=\"mailto:john@uplastech.com\">request a written quotation<\/a>.<\/p>\n<\/div>\n<\/div>\n<p><script type=\"application\/ld+json\">{\"@context\": \"https:\/\/schema.org\", \"@type\": \"FAQPage\", \"mainEntity\": [{\"@type\": \"Question\", \"name\": \"Why calibrate the cut gauge?\", \"acceptedAnswer\": {\"@type\": \"Answer\", \"text\": \"A drifting gauge pushes cut lengths to the tolerance edge, so bars come back long at one end and short at the other. Calibration keeps the error centred.\"}}, {\"@type\": \"Question\", \"name\": \"How much does the drift cost?\", \"acceptedAnswer\": {\"@type\": \"Answer\", \"text\": \"Using illustrative assumptions sorting and re-cutting costs 9 h and a hold. These are worked example values, not a measured series.\"}}, {\"@type\": \"Question\", \"name\": \"What tolerance applies?\", \"acceptedAnswer\": {\"@type\": \"Answer\", \"text\": \"A stated 1.0 mm cut-length tolerance. In this illustrative case the worst check reads 1.3 mm, over the line.\"}}, {\"@type\": \"Question\", \"name\": \"Why centre the band?\", \"acceptedAnswer\": {\"@type\": \"Answer\", \"text\": \"A shared band lets the bar sit at either edge; centring it removes the edge drift that causes the dispute.\"}}, {\"@type\": \"Question\", \"name\": \"Who owns the gauge?\", \"acceptedAnswer\": {\"@type\": \"Answer\", \"text\": \"A named programme owner re-calibrates on schedule. Without one owner the date is missed.\"}}, {\"@type\": \"Question\", \"name\": \"Does the rule expire?\", \"acceptedAnswer\": {\"@type\": \"Answer\", \"text\": \"It is valid until the re-calibration date. Keeping the schedule current keeps the cut evidence current.\"}}]}<\/script><\/p>\n","protected":false},"excerpt":{"rendered":"<p>This article quantifies the length error by gauge check, sets the calibration and band, and writes the rule into the cut plan.<\/p>","protected":false},"author":1,"featured_media":9736,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[17],"tags":[],"class_list":["post-9738","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-plastic-extrusion-process"],"meta_box":{"post-to-quiz_to":[]},"_links":{"self":[{"href":"https:\/\/uplastech.com\/ru\/wp-json\/wp\/v2\/posts\/9738","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/uplastech.com\/ru\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/uplastech.com\/ru\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/uplastech.com\/ru\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/uplastech.com\/ru\/wp-json\/wp\/v2\/comments?post=9738"}],"version-history":[{"count":1,"href":"https:\/\/uplastech.com\/ru\/wp-json\/wp\/v2\/posts\/9738\/revisions"}],"predecessor-version":[{"id":10043,"href":"https:\/\/uplastech.com\/ru\/wp-json\/wp\/v2\/posts\/9738\/revisions\/10043"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/uplastech.com\/ru\/wp-json\/wp\/v2\/media\/9736"}],"wp:attachment":[{"href":"https:\/\/uplastech.com\/ru\/wp-json\/wp\/v2\/media?parent=9738"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/uplastech.com\/ru\/wp-json\/wp\/v2\/categories?post=9738"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/uplastech.com\/ru\/wp-json\/wp\/v2\/tags?post=9738"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}