The problem

Symptom. A first-article report covers only cavity 1 of an 8-cavity tool, but the customer requires every cavity dimension signed off before series release.

What it costs. When a downstream cavity drifts, an illustrative 3 shifts of sorting and a 2 % scrap allowance are needed before the real cavity balance is known.

This article quantifies the coverage gap, sets the full-cavity requirement, and writes the cavity map into the first-article report so no cavity is left unverified.

When the first article covers only one cavity

In one illustrative first article an 8-cavity tool is reported from cavity 1 only, so the customer sees 12 of 96 cavity dimensions and signs off blind to the other seven. A later cavity drift is then discovered only after parts reach the line.

FAI trigger What it hides First figure to check
Only cavity 1 measured 7 of 8 cavities unseen Dimensions reported vs 96
No cavity map in report Balance spread unknown Worst-cavity deviation
Downstream drift found Illustrative 3-shift sort Scrap allowance 2 %
Sign-off rushed Series released blind Cavity count of the tool

Table 1 - Reading a single-cavity first-article before series release

Record which of these you are actually seeing before changing any setting. Two faults can look identical on the line and need opposite corrections.

Need a fixed price for this moulded part?

Send the 2D drawing, resin grade and annual volume. Our engineers return a DFM review, a material recommendation and a written quotation you can compare line by line.

Get a moulding quotationEmail [email protected]WhatsApp

Quantify the coverage gap across eight cavities

Size the gap before release. Measuring 1, 2, 4, 6 then 8 cavities reports an illustrative 12, 25, 50, 75 and 100 % of dimensions; the single-cavity report therefore hides 88 % of the picture. These are illustrative worked values from stated assumptions, not a measured series or a quoted result.

A five-step diagnostic sequence

  1. Measure cavity 1 first.
    Record the 12 dimensions at cavity 1 to confirm the method before the sweep.
  2. Sweep cavities 2 to 8.
    Repeat the 12 dimensions on every cavity so all 96 points are on the map.
  3. Compare the balance.
    Flag any cavity whose spread exceeds the stated band before sign-off.
  4. Reserve the allowance.
    Hold an illustrative 2 % scrap allowance against the worst cavity in the report.
  5. File the cavity map.
    Attach one row per cavity so the customer sees the full tool, not cavity 1.

The chart below is a typical result from that measurement step. Use it to separate a design limit from a setting that can still be recovered.

Cavity-by-Cavity Dimension Reporting at First Article: calculated response trend and an illustrative root-cause split
Figure 1 — Calculated response trend and an illustrative root-cause split. Values are engineering guidance for diagnosis, not a measured survey; confirm them on your own line before changing a drawing or a specification.

Set the full-cavity reporting requirement

Set the requirement at full cavity coverage with a balance check. With 8 cavities the report must show all 96 points plus an illustrative 2 % scrap allowance reserved for the worst cavity. These are illustrative worked values from stated assumptions, not a market survey, a quoted price or a measured series.

Clause or parameter Agreed value What goes wrong outside it
Cavity coverage All 8 cavities mapped 7 cavities released blind
Balance check Worst cavity flagged Drift found on the line
Scrap allowance 2 % worst cavity Sort cost blows up
Re-map on tooling Every tool change Balance lost after move

Table 2 - Cavity-reporting clauses for the first-article report

A controlled first-article measurement sequence

Run the measurement in a fixed order: measure cavity 1, confirm the method, sweep cavities 2 to 8, then compare the balance. The table ranks the actions by release risk so the cavity map is never skipped under schedule pressure.

Control action What it fixes Cost or trade-off
Map all 8 cavities Full dimension coverage Extra measurement time
Add balance check Catches worst cavity One row per cavity
Reserve 2 % allowance Covers worst cavity Scrap cost held
Re-map after tooling No drift after change One owner to maintain

Table 3 - Cavity-coverage controls ranked by release risk

Myth: "A process adjustment will fix it." Once a design limit is reached, more tuning only adds cost and variation. Confirm the limit with a measurement, then change the drawing or the specification.

Write the cavity map into the FAI report

Put the cavity map in the first-article report: one row per cavity, the 12 dimensions, and the balance spread. A written map turns a single-cavity sign-off into a tool-wide release the customer can trust.

Not sure whether the fault is in the tool or the process?

Send us the drawing, the process window and a few sample parts. We will tell you which change fixes the fault before you commit to a tool modification.

What to send us

  • Part drawing with the affected dimension
  • Current process settings
  • Sample parts from a good and a bad batch
  • Annual volume

Send the part for review

Keep the cavity balance current after tooling changes

Re-measure the balance after any tooling change, record the 2 % allowance actually used, and re-forecast the cavity spread. A written map reviewed on dated evidence settles the coverage question at first article rather than on the line.

Validate one change at a time and keep the measurement record. A supplier discussion backed by data is resolved in days, not weeks.

Before you release this injection moulding job

  • The first-article report maps all 8 cavities, not only cavity 1
  • The 12 dimensions are recorded on every cavity for full coverage
  • A balance check flags the worst cavity before series release
  • A 2 % scrap allowance is reserved against the worst cavity
  • The cavity map is re-run after any tooling or process change

Attach this list to the RFQ. Most moulding faults are decided at the drawing stage.

Why report every cavity?

An 8-cavity tool can drift on one cavity while the rest stay true. A cavity-1 report hides 88 % of the picture, so a downstream cavity fails only after parts reach the line.

How much does single-cavity hide?

Using illustrative assumptions, 1 of 8 cavities reports 12 % of dimensions; the remaining 88 % is unseen until a drift is found in production.

What is the balance check?

It compares the spread of all 8 cavities and flags the worst one. With 8 cavities an illustrative 2 % scrap allowance is reserved against that cavity.

Can we sample cavities?

Only if the customer agrees a reduced plan. The default requirement is full cavity coverage with a balance check at first article.

Who owns the cavity map?

A named owner re-runs it after tooling changes. Without one owner the balance is lost the moment the tool is touched.

Does the map expire?

It is valid until the tool or process changes. Re-mapping at each change keeps the evidence current without re-measuring every lot.

Get a mouldable part and a fixed quotation

Send us the part file and the failure history. Our engineers will return a DFM review, a material recommendation and a fixed quotation with a defined first-article acceptance test.

To get an accurate quote, send:

  • 3D file or 2D part drawing
  • Resin grade and any regrind limit
  • Annual volume and target unit price
  • The failed sample or defect photos

Request a DFM review and quote

Prefer to talk it through first?

Correio eletrónico [email protected] or message us on WhatsApp +86 177 1752 9949. Send a drawing, a sample or a specification and an engineer will reply.

Why buyers work with Uplastech

ISO 9001, ISO 14001 and ISO 45001 certified. Founded in 2016, with injection moulding lines in Shanghai and an extrusion plant in Jiangsu. Moulding machines from 90T to 1100T and a maximum shot weight of 5100 g. Samples and a written quotation are available on request.

Hi there! I'm John, dad and hero to awesome kid. By day, I'm a plastics manufacturing vet — injection molding, extrusion and vacuum forming — who went from factory floors to technical management. Here to share what I've learned—let's grow together!
pt_PTPT

Pedir um orçamento rápido

Enviar desenhos e requisitos pormenorizados através de

Emial: [email protected]

Ou preencha o formulário de contacto abaixo: