Top 5 Plastic Vacuum Forming Factories in Belgium

Workers in safety gear on a factory floor with machinery and pallets

Plastic vacuum forming is a versatile manufacturing process1 that shapes heated plastic sheets over molds using a vacuum, creating lightweight, cost-effective parts for industries like packaging, automotive, and medical.

Vacuum forming uses heat and suction to mold plastic sheets2 into precise shapes, offering an affordable solution for custom parts in packaging, automotive, and industrial applications.

Belgium, with its robust manufacturing sector, hosts several top-tier 진공 성형3 factories. This article explores the leading five, their services, and the technology behind vacuum forming, helping you understand its applications and benefits.

Vacuum forming is a cost-effective manufacturing process.True

It uses inexpensive molds and is ideal for low to medium production runs, reducing overall costs.

Vacuum forming is only suitable for small parts.False

It excels at producing large parts like machine covers and automotive components, not just small items.

Who Are the Top 5 Plastic Vacuum Forming Factories in Belgium?

Belgium’s vacuum forming industry thrives on innovation and quality. Here are the top five factories, renowned for their expertise and diverse offerings.

Workers in protective clothing operate machinery in a spacious, well-lit factory interior
Vacuum Forming Factories

Belgium’s top vacuum forming factories—BTL Plastics, Vitalo Group, AB Flexibles, ABS Plastics NV, and C.M.K. Kunststoffen—deliver high-quality, custom plastic solutions4 for global industries.

Factory Name Location Year Founded Employees Main Services
BTL Plastics Wielsbeke, Belgium 2002 21-100 Thermoforming for industrial vehicles, machine covers
Vitalo Group Meulebeke, Belgium 1936 501-1000 Thermoforming for insulation solutions
AB Flexibles Kuurne, Belgium Not specified 31-100 Vacuum forming packaging, 열성형5 films
ABS Plastics NV Zedelgem, Belgium 1968 51-200 진공 성형
C.M.K. Kunststoffen Hamont-Achel, Belgium 1995 51-200 Thermoforming, injection molding

BTL Plastics

Located in Wielsbeke, BTL Plastics specializes in parts for industrial vehicles and machinery, leveraging automation for precision and efficiency.

Vitalo Group

Based in Meulebeke, Vitalo Group excels in thermoforming plastics and foams for acoustic and thermal insulation, serving industries needing advanced material solutions.

Workers in a manufacturing plant operating machinery and assembling products
Vacuum Forming Factories

AB Flexibles

In Kuurne, AB Flexibles focuses on packaging, offering thermoformed films and vacuum-formed solutions tailored to client needs.

ABS Plastics NV

Operating from Zedelgem since 1968, ABS Plastics NV provides reliable vacuum forming services with decades of expertise.

Workers in protective gear at a factory production line with white plastic molds
Vacuum Forming Factories

C.M.K. Kunststoffen

Located in Hamont-Achel, C.M.K. Kunststoffen combines thermoforming and injection molding for versatile manufacturing options.

All top Belgian vacuum forming factories focus solely on packaging.False

While some like AB Flexibles specialize in packaging, others like BTL Plastics and Vitalo Group serve industrial and insulation sectors.

What is Plastic Vacuum Forming?

Vacuum forming is a cornerstone of modern manufacturing, offering flexibility and efficiency.

Vacuum forming heats thermoplastic sheets, shapes them over molds with a vacuum, and cools them into durable parts for diverse applications.

번호가 표시된 CNC 기계에서 파란색 패널을 성형하는 모습
Vacuum Forming process

Common Materials Used

Common thermoplastics include:

  • ABS: High impact resistance for automotive parts.

  • HIPS: Economical for packaging.

  • PE: Durable for containers.

  • PP: Chemical-resistant for medical uses.

A blue panel being shaped on a CNC machine with numbered markingsRolls of BOPP film being manufactured in a factory setting
Vacuum Forming Sheets

  • PVC: Versatile for displays.

  • 아크릴(PMMA): Transparent for signage.

  • 폴리카보네이트(PC): Strong for safety shields.

재료 주요 속성 Typical Use
ABS Impact resistance Automotive components
HIPS Cost-effective Packaging trays
폴리카보네이트 High strength Safety shields

ABS is widely used in vacuum forming.True

Its durability and impact resistance make it ideal for structural parts like dashboards.

What Are the Steps in the Vacuum Forming Process?

The vacuum forming process is straightforward yet precise, enabling rapid production of custom parts.

Vacuum forming involves heating plastic, shaping it with a vacuum over a mold, and cooling it into a finished part, ideal for prototyping and production.

운송 및 보관용 검은색 손잡이 트레이
진공 성형 제품

Process Steps

  1. 난방: Plastic sheet heated to 150-200°C.

  2. 형성: Sheet stretched over mold; vacuum applied.

  3. 냉각: Part cooled to solidify shape.

  4. 트리밍: Excess plastic removed.

  5. 마무리: Additional operations like drilling completed.

Vacuum forming is slow and inefficient.False

It offers rapid production cycles, making it efficient for prototyping and medium runs.

What Are the Key Factors in Vacuum Forming?

Success in vacuum forming hinges on controlling critical variables.

Vacuum forming depends on material choice, mold design, and process parameters like temperature and vacuum strength, affecting part quality and cost.

키보드 스위치를 고정하는 데 사용되는 다양한 흑백 플라스틱 트레이
진공 성형 제품

재료 선택

Material properties (e.g., thickness, UV resistance) dictate suitability. Thicker sheets allow deeper draws but raise costs.

금형 설계

Molds must include draft angles (1-2°) and avoid sharp corners to ensure easy removal and uniform thickness.

온도 제어

Precise heating ensures pliability without degrading the plastic.

Material choice impacts vacuum forming outcomes.True

Different plastics offer unique properties, influencing strength, flexibility, and application.

What Are the Applications of Vacuum Forming?

Vacuum forming serves a wide range of industries with tailored solutions.

Vacuum forming produces parts for automotive, medical, packaging, consumer goods, and industrial uses, balancing cost and performance.

나무 표면에 독특한 세로 슬라이스 디자인의 흰색 아이스 큐브 트레이 2개
진공 성형 제품

  • 자동차: Dashboards, trim.

  • 의료: Device enclosures, sterile packaging.

  • 패키징: Blister packs, trays.

  • 소비재: Toys, displays.

  • Industrial: Machine covers.

Vacuum forming is limited to prototyping.False

It’s used for both prototypes and production parts across industries.

How Does Vacuum Forming Compare to Other Methods?

Vacuum forming stands out but has trade-offs compared to alternatives.

일반 배경에 세 가지 크기의 플라스틱 블리스터 포장재 제공
진공 성형 제품

Vacuum forming excels in cost and speed for large parts but lacks the precision of injection molding for complex designs.

방법 장점 단점
진공 성형 Cost-effective, large parts Limited to single-sided molds
사출 성형 High precision, complex parts Expensive molds, high volume
블로우 성형 Hollow parts Limited shapes

Vacuum forming is less precise than injection molding.True

It struggles with tight tolerances and intricate details.

결론

Belgium’s top vacuum forming factories—BTL Plastics, Vitalo Group, AB Flexibles, ABS Plastics NV, and C.M.K. Kunststoffen—offer specialized solutions6 for diverse needs. Vacuum forming’s affordability7, speed, and versatility make it a go-to process for industries worldwide. Whether you’re designing packaging or industrial components, understanding this technology can unlock efficient manufacturing options.


  1. Learn about the manufacturing process of vacuum forming to appreciate its efficiency and versatility in creating custom parts. 

  2. Discover how plastic sheets are integral to vacuum forming, enhancing your knowledge of this manufacturing technique. 

  3. Explore this link to gain a deeper understanding of vacuum forming, its applications, and benefits in various industries. 

  4. Discover the process behind custom plastic solutions and how they cater to specific industry needs, ensuring quality and innovation. 

  5. Learn about thermoforming techniques and their applications in creating diverse products, crucial for many manufacturing sectors.benefits in various industries. 

  6. Learn about specialized solutions that can cater to unique manufacturing needs, improving efficiency and product quality. 

  7. Discover insights on how affordability in manufacturing can lead to better resource allocation and increased competitiveness. 

최신 게시물

WhatsApp
Facebook
트위터
LinkedIn
Pinterest
안녕하세요! 저는 멋진 아이의 아빠이자 영웅인 John입니다. 저는 낮에는 공장 현장에서 기술 관리자로 일한 플라스틱 압출 업계의 베테랑입니다. 제가 배운 것을 공유하며 함께 성장해 봅시다!
ko_KRKO

빠른 견적 요청하기

다음을 통해 도면 및 세부 요구 사항을 보내주세요.

Emial: uplastech@gmail.com

또는 아래 문의 양식을 작성하세요: