{"id":7706,"date":"2025-08-31T09:00:00","date_gmt":"2025-08-31T08:00:00","guid":{"rendered":"https:\/\/uplastech.com\/packing-shipping-extruded-profiles\/"},"modified":"2025-08-31T09:00:00","modified_gmt":"2025-08-31T08:00:00","slug":"packing-shipping-extruded-profiles","status":"publish","type":"post","link":"https:\/\/uplastech.com\/fr\/packing-shipping-extruded-profiles\/","title":{"rendered":"Packing and Shipping Extruded Profiles: Bundles, Containers and Claims"},"content":{"rendered":"<style>\n.upl-blog{font-size:17px;line-height:1.78;color:#1f2937}\n.upl-blog p{margin:0 0 18px}\n.upl-blog h2{font-size:26px;line-height:1.3;color:#0b2b33;margin:46px 0 14px;font-weight:700;letter-spacing:-.015em}\n.upl-blog h3{font-size:19.5px;color:#0d3b47;margin:28px 0 10px;font-weight:700}\n.upl-blog ul,.upl-blog ol{margin:0 0 20px;padding-left:22px}\n.upl-blog li{margin:0 0 9px}\n.upl-blog figure{margin:0 0 34px}\n.upl-blog figure img{width:100%;height:auto;display:block;border-radius:10px}\n.upl-blog figcaption{font-size:13px;color:#6b7280;margin-top:10px;line-height:1.5}\n.upl-blog .toc{background:none;border:0;border-radius:0;padding:0;margin:0 0 34px}\n.upl-blog .toc .lwptoc{margin:0}\n.upl-blog .toc h4{margin:0 0 10px;font-size:13px;letter-spacing:.1em;text-transform:uppercase;color:#0d5563}\n.upl-blog .toc ol{margin:0;padding-left:18px;font-size:14.5px}\n.upl-blog .toc li{margin-bottom:6px}\n.upl-blog table{width:100%;border-collapse:collapse;font-size:14.5px;margin:0 0 10px}\n.upl-blog th{background:#0d3b47;color:#fff;text-align:left;padding:11px 13px;font-weight:600;font-size:13.5px;border:0}\n.upl-blog td{padding:11px 13px;border:0;border-bottom:1px solid #e8ebed;vertical-align:top}\n.upl-blog tbody tr:nth-child(even){background:#fafbfc}\n.upl-blog .tablecap{font-size:12.5px;color:#6b7280;margin:0 0 30px}\n.upl-blog .myth{background:#fff8ef;border:1px solid #f6ddbd;border-radius:8px;padding:16px 20px;margin:0 0 26px;font-size:15.5px}\n.upl-blog .myth b{color:#a85c10}\n.upl-blog .callout{background:#f2f8f9;border-radius:8px;padding:18px 22px;margin:0 0 26px;font-size:15.5px;border-left:3px solid #14707f}\n.upl-blog .faq h3{border-top:1px solid #eceff1;padding-top:22px;margin-top:0;font-size:18px}\n.upl-blog .faq h3:first-of-type{border-top:0;padding-top:0}\n.upl-blog .cta{background:linear-gradient(135deg,#0b2b33,#0d5563);color:#fff;border-radius:12px;padding:34px;margin:48px 0 30px}\n.upl-blog .cta h2,.upl-blog .cta .cta-h{color:#fff;margin:0 0 10px;font-size:24px;font-weight:700;line-height:1.3}\n.upl-blog .cta p{color:#c9dee3;margin:0 0 20px;font-size:16px}\n.upl-blog .btn{display:inline-block;background:#e07a1f;color:#fff;text-decoration:none;font-weight:700;padding:13px 26px;border-radius:8px;font-size:15.5px}\n.upl-blog .rel{border-top:1px solid #e8ebed;margin-top:40px;padding-top:26px}\n.upl-blog .rel h4{font-size:13px;letter-spacing:.1em;text-transform:uppercase;color:#6b7280;margin:0 0 14px}\n.upl-blog .rel ul{list-style:none;padding:0;margin:0}\n.upl-blog .rel li{padding:11px 0;border-bottom:1px dashed #e8ebed}\n.upl-blog .rel a{text-decoration:none;font-weight:600;font-size:15.5px}\n@media(max-width:640px){.upl-blog h2{font-size:22px}.upl-blog table{font-size:13px}.upl-blog .cta{padding:24px}}\n\/* \u5355\u7bc7\u9875\u9690\u85cf WhatsApp \u81ea\u52a8\u5c55\u5f00\u7684\u95ee\u5019\u5361\uff0c\u53ea\u4fdd\u7559\u5706\u5f62\u6c14\u6ce1\uff0c\u907f\u514d\u906e\u6321\u4fa7\u680f\u8be2\u76d8\u63d0\u4ea4\u6309\u94ae *\/\nbody.single-post .ht_ctc_chat_greetings_box{display:none !important}\n<\/style>\n<div class=\"upl-blog\">\n<figure>\n<img fetchpriority=\"high\" decoding=\"async\" src=\"https:\/\/uplastech.com\/wp-content\/uploads\/2026\/10\/packing-shipping-extruded-profiles.jpg\" alt=\"Bundled plastic profiles strapped and stacked ready for container loading at a factory\" width=\"1536\" height=\"909\"><figcaption>Packing is the last operation and the first thing the customer sees. It is also where a profile that passed every inspection arrives bent, scuffed or short.<\/figcaption><\/figure>\n<div class=\"toc\"><\/div>\n<h2 id=\"cost\">Why packing costs more than people think<\/h2>\n<p>Packing is usually quoted as a line item of a few percent and then treated as an afterthought. In reality it carries three separate costs: the materials and labour, the freight volume it consumes, and the scrap it prevents or fails to prevent.<\/p>\n<table>\n<thead>\n<tr>\n<th>Composant<\/th>\n<th>Typical share of delivered price<\/th>\n<th>Where it goes wrong<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>Packaging material<\/td>\n<td>0.5 \u2013 1.5%<\/td>\n<td>Over-specified film; under-specified corners<\/td>\n<\/tr>\n<tr>\n<td>Packing labour<\/td>\n<td>0.5 \u2013 2%<\/td>\n<td>Manual bundling at high volume<\/td>\n<\/tr>\n<tr>\n<td>Freight volume penalty<\/td>\n<td>1 \u2013 6%<\/td>\n<td>Bundles that do not fill the container<\/td>\n<\/tr>\n<tr>\n<td>Damage and claims<\/td>\n<td>0.5 \u2013 4%<\/td>\n<td>Insufficient interleaving, no end protection<\/td>\n<\/tr>\n<tr>\n<td>Handling at the customer<\/td>\n<td>Not visible<\/td>\n<td>Bundles too heavy for the receiving area<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p class=\"tablecap\">Table 1 \u2014 Where packing cost actually sits. The freight volume penalty is usually the largest single item and the one least examined.<\/p>\n<div class=\"callout\">\n<p><strong>The cheapest packing is the one that fills the container.<\/strong> A 6 m profile shipped in a 40 ft container has 12.03 m of internal length; a bundle that wastes 400 mm at each end costs 7% of the freight bill on every shipment, forever.<\/p>\n<\/div>\n<h2 id=\"threats\">Protection: what you are protecting against<\/h2>\n<p>Before choosing materials, list the actual damage modes for the specific profile. A rigid PVC window profile and a soft PVC tube have almost nothing in common beyond both being extruded.<\/p>\n<table>\n<thead>\n<tr>\n<th>Damage mode<\/th>\n<th>What it looks like<\/th>\n<th>Protection<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>Abrasion in transit<\/td>\n<td>Scuffed or polished faces, matt patches<\/td>\n<td>Interleaving film or paper between profiles<\/td>\n<\/tr>\n<tr>\n<td>Point loading<\/td>\n<td>Flat spots, dents at strap positions<\/td>\n<td>Corner protectors, wider straps, edge board<\/td>\n<\/tr>\n<tr>\n<td>Bending under stack load<\/td>\n<td>Permanent bow after unpacking<\/td>\n<td>Support at 1 m intervals; limit stack height<\/td>\n<\/tr>\n<tr>\n<td>End damage<\/td>\n<td>Chipped or crushed ends<\/td>\n<td>End caps, end board, recessed bundling<\/td>\n<\/tr>\n<tr>\n<td>UV during storage<\/td>\n<td>Yellowing, chalking on exposed faces<\/td>\n<td>Opaque wrap or indoor storage<\/td>\n<\/tr>\n<tr>\n<td>Moisture and condensation<\/td>\n<td>Water marks, mould between profiles<\/td>\n<td>Vented wrap, desiccant for long sea freight<\/td>\n<\/tr>\n<tr>\n<td>Contamination<\/td>\n<td>Dust, oil, grit bonded to the surface<\/td>\n<td>Sealed wrap; clean packing area<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p class=\"tablecap\">Table 2 \u2014 Damage modes and their countermeasures. Most claims come from the first two rows, and both are cheap to prevent.<\/p>\n<p>The order of priority is abrasion first, point loading second, everything else a distant third. A profile that has rubbed against its neighbour for 6,000 km will arrive with a surface that no amount of cleaning fixes, and that is a total loss on a visible part.<\/p>\n<h2 id=\"bundle\">Bundle design<\/h2>\n<p>A bundle is a structural unit. It has to survive being lifted by forklift, stacked three high and dropped 100 mm onto a dock. The design variables are the number of profiles, the strap positions, the interleaving and the end protection.<\/p>\n<table>\n<thead>\n<tr>\n<th>Profile type<\/th>\n<th>Bundle size<\/th>\n<th>Strap spacing<\/th>\n<th>Bundle weight<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>Window profile, 6 m<\/td>\n<td>20 \u2013 30 pieces<\/td>\n<td>1.2 \u2013 1.5 m<\/td>\n<td>250 \u2013 400 kg<\/td>\n<\/tr>\n<tr>\n<td>Technical profile, 3 m<\/td>\n<td>40 \u2013 60 pieces<\/td>\n<td>0.8 \u2013 1.0 m<\/td>\n<td>200 \u2013 350 kg<\/td>\n<\/tr>\n<tr>\n<td>Pipe and conduit, 6 m<\/td>\n<td>Hexagonal pack<\/td>\n<td>1.5 m<\/td>\n<td>300 \u2013 500 kg<\/td>\n<\/tr>\n<tr>\n<td>Small tube, 2 m<\/td>\n<td>Carton or tube<\/td>\n<td>n\/a<\/td>\n<td>15 \u2013 30 kg<\/td>\n<\/tr>\n<tr>\n<td>Rod, 3 m<\/td>\n<td>20 \u2013 40 pieces<\/td>\n<td>1.0 m<\/td>\n<td>150 \u2013 400 kg<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p class=\"tablecap\">Table 3 \u2014 Typical bundle configurations. Keeping bundles under 500 kg keeps them within the capacity of a standard forklift with the mast extended.<\/p>\n<p>Strap tension is the detail that decides whether a bundle arrives square. Too loose and the profiles shuffle and abrade; too tight and the strap cuts into the profile at the corners. For hollow profiles, straps should sit over a rigid web rather than spanning an open cavity, or the wall will collapse.<\/p>\n<p>Stacking is the other half. Bundles stacked more than three high put the bottom bundle under a load it was not designed for, and profiles creep under sustained load at ambient temperature. If the warehouse stacks five high, the bundle design has to be specified for five high.<\/p>\n<h2 id=\"surface\">Interleaving and surface protection<\/h2>\n<table>\n<thead>\n<tr>\n<th>Option<\/th>\n<th>Protection level<\/th>\n<th>Co\u00fbt<\/th>\n<th>Meilleur pour<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>Nothing<\/td>\n<td>None<\/td>\n<td>\u2014<\/td>\n<td>Hidden profiles, rough handling acceptable<\/td>\n<\/tr>\n<tr>\n<td>PE interleaving film<\/td>\n<td>Good against abrasion<\/td>\n<td>Faible<\/td>\n<td>Most visible profiles<\/td>\n<\/tr>\n<tr>\n<td>Foam interleaving<\/td>\n<td>Very good, cushions point loads<\/td>\n<td>Moyen<\/td>\n<td>Textured or high-gloss surfaces<\/td>\n<\/tr>\n<tr>\n<td>Protective tape on the face<\/td>\n<td>Good, but removal labour<\/td>\n<td>Moyen<\/td>\n<td>High-gloss, small parts<\/td>\n<\/tr>\n<tr>\n<td>Shrink wrap per bundle<\/td>\n<td>Good against dirt and moisture<\/td>\n<td>Moyen<\/td>\n<td>Sea freight<\/td>\n<\/tr>\n<tr>\n<td>Individual bagging<\/td>\n<td>Best<\/td>\n<td>Haut<\/td>\n<td>Medical, clean-room, retail<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p class=\"tablecap\">Table 4 \u2014 Surface protection options. Interleaving film is the default for anything visible; the rest are for specific risks.<\/p>\n<p>The choice is usually driven by what the customer does with the part. A profile that goes straight into an assembly jig needs only abrasion protection. A profile that is displayed, or handled by an end user, needs surface protection that survives the whole journey and comes off cleanly.<\/p>\n<p>Adhesive tape is the option people regret. It works, but removal is labour the customer pays for, and if the tape stays on through a hot container the adhesive transfers. Where tape is used, specify a low-tack grade and a maximum dwell time.<\/p>\n<h2 id=\"container\">Length, weight and container loading<\/h2>\n<p>Container loading is where packing decisions turn into money. A 40 ft high-cube container has 12.03 m of internal length, 2.35 m of width and 2.69 m of height. Every millimetre of that length that a bundle does not use is paid for and not used.<\/p>\n<table>\n<thead>\n<tr>\n<th>Profile length<\/th>\n<th>Loading arrangement<\/th>\n<th>Length utilisation<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>6,000 mm<\/td>\n<td>Two rows end to end<\/td>\n<td>99.7%<\/td>\n<\/tr>\n<tr>\n<td>5,800 mm<\/td>\n<td>Two rows, 430 mm wasted<\/td>\n<td>96.4%<\/td>\n<\/tr>\n<tr>\n<td>4,000 mm<\/td>\n<td>Three rows, 30 mm wasted<\/td>\n<td>99.8%<\/td>\n<\/tr>\n<tr>\n<td>3,000 mm<\/td>\n<td>Four rows<\/td>\n<td>99.7%<\/td>\n<\/tr>\n<tr>\n<td>2,500 mm<\/td>\n<td>Four rows plus 2,030 mm of other goods<\/td>\n<td>Needs mixed load<\/td>\n<\/tr>\n<tr>\n<td>6,500 mm<\/td>\n<td>Cannot load in a 40 ft container<\/td>\n<td>\u2014<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p class=\"tablecap\">Table 5 \u2014 Length utilisation by profile length. 5.8 m is a surprisingly expensive length because it wastes 430 mm per row.<\/p>\n<p>Weight is the other limit. A 40 ft container is rated for about 26\u201328 tonnes of payload, and a bundle of rigid PVC profile at 1.4 g\/cm\u00b3 fills the volume long before it reaches that. For dense profiles \u2014 filled compounds, thick rod \u2014 weight becomes the binding constraint and the loading plan has to be built around it.<\/p>\n<p>The 6.5 m profile in the table is a real design constraint worth flagging early: if a profile is longer than about 5.9 m, it cannot be shipped in a standard container and has to go break-bulk or in a 45 ft container, which changes the freight cost by a large multiple.<\/p>\n<h2 id=\"tubes\">Packaging tubes and small profiles<\/h2>\n<p>Small profiles cannot be bundled \u2014 there are too many pieces and they are too light. The standard answer is a packaging tube: a rigid or semi-rigid tube, usually extruded from the same plant, with end caps.<\/p>\n<table>\n<thead>\n<tr>\n<th>Tube type<\/th>\n<th>Diameter range<\/th>\n<th>Meilleur pour<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>Rigid PVC tube with caps<\/td>\n<td>40 \u2013 200 mm<\/td>\n<td>Long thin profiles, rods<\/td>\n<\/tr>\n<tr>\n<td>Thin-wall PE tube<\/td>\n<td>25 \u2013 100 mm<\/td>\n<td>Light profiles, one-trip<\/td>\n<\/tr>\n<tr>\n<td>Cardboard core with wrap<\/td>\n<td>50 \u2013 150 mm<\/td>\n<td>Flexible profiles, seals<\/td>\n<\/tr>\n<tr>\n<td>Corrugated carton, long<\/td>\n<td>Any<\/td>\n<td>Short lengths, mixed items<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p class=\"tablecap\">Table 6 \u2014 Packaging tube options. The rigid PVC tube is the most protective and is usually made on the same extrusion line that made the product.<\/p>\n<p>Tube length should be 50\u2013100 mm longer than the contents so the caps do not press on the ends. Tube wall thickness matters more than people expect: a thin-wall tube deforms in a stack and transfers the load to the contents, which defeats the purpose.<\/p>\n<h2 id=\"marking\">Marking and documentation<\/h2>\n<p>Every bundle needs four pieces of information visible without opening it: part number, quantity, length and batch. A fifth \u2014 the production date \u2014 is worth adding because it lets the customer apply first-in-first-out without opening anything.<\/p>\n<p>Labels should go on the outside of the wrap and on a card inside the bundle, because the outer label is the one that gets torn off in transit. Where the customer's receiving system scans barcodes, agree the label format and position before the first shipment rather than after the first rejection.<\/p>\n<h2 id=\"claims\">Damage claims and inspection<\/h2>\n<p>Damage claims are won or lost on the packing specification and the shipping photographs, not on the argument afterwards. A specification that states the interleaving, the strap spacing, the stack limit and the end protection gives both sides something to check against.<\/p>\n<p>Photograph every bundle at loading, with the label visible, and photograph the container floor and walls before loading. That takes two minutes and settles most disputes about who caused a dent. Where the shipment is high value, a third-party inspection at loading costs very little relative to the value of the claim it prevents.<\/p>\n<div class=\"faq\">\n<h3>How should extruded profiles be packed?<\/h3>\n<p>Bundled with interleaving film between profiles, strapped at 1.0\u20131.5 m intervals with corner protection, end caps on, and labelled on the outside. Stack no more than three high unless the bundle is designed for more.<\/p>\n<h3>Why do my profiles arrive scuffed?<\/h3>\n<p>Abrasion between profiles in transit. Interleaving film is the fix, and it is cheap. If the scuffing is only at the strap positions, the strap tension is too high or the strap is spanning an open cavity.<\/p>\n<h3>What is the best length for container shipping?<\/h3>\n<p>6,000 mm, because two rows fill a 40 ft container almost exactly. 5,800 mm wastes 430 mm per row, which is about 3.6% of the freight bill on every shipment for no benefit.<\/p>\n<h3>How heavy should a bundle be?<\/h3>\n<p>Under 500 kg. That keeps it within a standard forklift's capacity with the mast extended and within what a receiving area can handle without special equipment. Heavier bundles need to be agreed with the customer.<\/p>\n<h3>Should profiles be shrink wrapped?<\/h3>\n<p>For sea freight, yes \u2014 it protects against dirt and condensation. For road freight in dry conditions, interleaving film plus strapping is usually enough and costs less.<\/p>\n<h3>How do I stop profiles bending in the warehouse?<\/h3>\n<p>Support them at intervals of about 1 m, limit the stack height to three bundles, and do not store them leaning against a wall. Thermoplastics creep under sustained load at room temperature, and a bend that develops over months is permanent.<\/p>\n<h3>What about packaging tubes for small profiles?<\/h3>\n<p>Use a rigid tube with 50\u2013100 mm of clearance beyond the contents so the caps do not load the ends. Thin-wall tubes deform in a stack and transfer load to the product, so specify the wall thickness rather than just the diameter.<\/p>\n<h3>How do I handle a damage claim?<\/h3>\n<p>Have a written packing specification, photograph every bundle at loading with the label visible, and inspect on arrival before signing. Claims are settled on that evidence, not on inspection after the goods have been moved twice.<\/p>\n<\/div>\n<div class=\"cta\">\n<p class=\"cta-h\">Shipping profiles overseas?<\/p>\n<p>Tell us the profile, the length, the volume and the destination. We will tell you the bundle configuration, the container loading plan and the packing specification that keeps the parts undamaged on arrival.<\/p>\n<p><a class=\"btn\" href=\"https:\/\/uplastech.com\/fr\/solutions-dextrusion-plastique\/\">Talk to an extrusion engineer<\/a>\n<\/div>\n<div class=\"rel\">\n<h4>Continue reading<\/h4>\n<ul>\n<li><a href=\"https:\/\/uplastech.com\/fr\/profile-cut-length-accuracy\/\">Profile Cut Length Accuracy<\/a><\/li>\n<li><a href=\"https:\/\/uplastech.com\/fr\/plastic-packaging-tube-extrusion\/\">Plastic Packaging Tube Extrusion<\/a><\/li>\n<li><a href=\"https:\/\/uplastech.com\/fr\/extrusion-quality-control\/\">Extrusion Quality Control: Inspection, SPC and Acceptance<\/a><\/li>\n<li><a href=\"https:\/\/uplastech.com\/fr\/profiles-en-pvc\/\">PVC Profiles: Extrusion, Design and Specification<\/a><\/li>\n<li><a href=\"https:\/\/uplastech.com\/fr\/profile-tolerance-secondary-operations\/\">Profile Tolerances and Secondary Operations<\/a><\/li>\n<\/ul>\n<\/div>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>Packing is where a profile that passed inspection arrives bent or scuffed. Bundle design, container length utilisation and the specification that prevents claims.<\/p>","protected":false},"author":1,"featured_media":7700,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_seopress_titles_title":"Packing and Shipping Extruded Profiles: Bundles, Containers","_seopress_titles_desc":"Packing is where a profile that passed inspection arrives bent or scuffed. Bundle design, container length utilisation and the specification that prevents","_seopress_robots_index":"","_seopress_robots_follow":"","_seopress_robots_imageindex":"","_seopress_robots_snippet":"","_seopress_robots_primary_cat":"17","_seopress_robots_breadcrumbs":"","_seopress_robots_freeze_modified_date":"","_seopress_robots_custom_modified_date":"","_seopress_robots_canonical":"","_seopress_social_fb_title":"","_seopress_social_fb_desc":"","_seopress_social_fb_img":"","_seopress_social_fb_img_attachment_id":0,"_seopress_social_fb_img_width":0,"_seopress_social_fb_img_height":0,"_seopress_social_twitter_title":"","_seopress_social_twitter_desc":"","_seopress_social_twitter_img":"","_seopress_social_twitter_img_attachment_id":0,"_seopress_social_twitter_img_width":0,"_seopress_social_twitter_img_height":0,"_seopress_redirections_value":"","_seopress_redirections_enabled":"","_seopress_redirections_enabled_regex":"","_seopress_redirections_logged_status":"","_seopress_redirections_param":"","_seopress_redirections_type":0,"_seopress_analysis_target_kw":"packing shipping extruded profiles","footnotes":""},"categories":[17,36],"tags":[],"class_list":["post-7706","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-plastic-extrusion-process","category-profile-extrusion"],"meta_box":{"post-to-quiz_to":[]},"_links":{"self":[{"href":"https:\/\/uplastech.com\/fr\/wp-json\/wp\/v2\/posts\/7706","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/uplastech.com\/fr\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/uplastech.com\/fr\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/uplastech.com\/fr\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/uplastech.com\/fr\/wp-json\/wp\/v2\/comments?post=7706"}],"version-history":[{"count":0,"href":"https:\/\/uplastech.com\/fr\/wp-json\/wp\/v2\/posts\/7706\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/uplastech.com\/fr\/wp-json\/wp\/v2\/media\/7700"}],"wp:attachment":[{"href":"https:\/\/uplastech.com\/fr\/wp-json\/wp\/v2\/media?parent=7706"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/uplastech.com\/fr\/wp-json\/wp\/v2\/categories?post=7706"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/uplastech.com\/fr\/wp-json\/wp\/v2\/tags?post=7706"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}