{"id":7320,"date":"2026-10-24T18:28:02","date_gmt":"2026-10-24T17:28:02","guid":{"rendered":"https:\/\/uplastech.com\/pc-injection-molding\/"},"modified":"2026-10-26T07:38:48","modified_gmt":"2026-10-26T07:38:48","slug":"pc-injection-molding","status":"publish","type":"page","link":"https:\/\/uplastech.com\/es\/pc-injection-molding\/","title":{"rendered":"Custom PC Injection Molding"},"content":{"rendered":"<style>\n.upl-page{font-size:17px;line-height:1.78;color:#1f2937}\n.upl-page p{margin:0 0 18px}\n.upl-page h1{font-size:38px;line-height:1.16;letter-spacing:-.025em;color:#0b2b33;margin:0 0 18px;font-weight:800}\n.upl-page h2{font-size:26px;line-height:1.3;color:#0b2b33;margin:48px 0 14px;font-weight:700;letter-spacing:-.015em}\n.upl-page h3{font-size:19px;color:#0d3b47;margin:26px 0 10px;font-weight:700}\n.upl-page ul,.upl-page ol{margin:0 0 20px;padding-left:22px}\n.upl-page li{margin:0 0 9px}\n.upl-page .lead{font-size:19px;line-height:1.65;color:#4b5563;margin:0 0 36px}\n.upl-page a{color:#0d6b7d}\n.upl-page strong{color:#0b2b33}\n.upl-page .sec-note{font-size:13px;color:#6b7280;margin:-4px 0 26px}\n.upl-page .stats{display:grid;grid-template-columns:repeat(auto-fit,minmax(180px,1fr));gap:16px;margin:0 0 20px}\n.upl-page .stat{background:#f7fafb;border:1px solid #e3ebee;border-left:3px solid #14707f;border-radius:8px;padding:16px 20px}\n.upl-page .stat b{display:block;font-size:24px;line-height:1.2;color:#0b2b33;letter-spacing:-.02em;margin-bottom:4px}\n.upl-page .stat span{font-size:12.5px;color:#6b7280;letter-spacing:.04em;text-transform:uppercase;font-weight:600}\n.upl-page .prod-grid{display:grid;grid-template-columns:repeat(auto-fill,minmax(300px,1fr));gap:26px;margin:0 0 16px}\n.upl-page .prod{background:#fff;border:1px solid #e6ebed;border-radius:12px;overflow:hidden;display:flex;flex-direction:column;scroll-margin-top:96px}\n.upl-page .prod img{width:100%;height:198px;object-fit:cover;display:block;background:#f2f5f6}\n.upl-page .prod .txt{padding:17px 20px 21px;flex:1}\n.upl-page .prod h3{margin:0 0 8px;font-size:17.5px;line-height:1.35;color:#0b2b33}\n.upl-page .prod p{margin:0;font-size:14.5px;color:#5b666b;line-height:1.62}\n.upl-page table{width:100%;border-collapse:collapse;font-size:14.5px;margin:0 0 10px}\n.upl-page th{background:#0d3b47;color:#fff;text-align:left;padding:11px 13px;font-weight:600;font-size:13.5px;border:0}\n.upl-page td{padding:11px 13px;border:0;border-bottom:1px solid #e8ebed;vertical-align:top}\n.upl-page tbody tr:nth-child(even){background:#fafbfc}\n.upl-page .tablecap{font-size:12.5px;color:#6b7280;margin:0 0 30px}\n.upl-page .callout{background:#f2f8f9;border-radius:8px;padding:18px 22px;margin:0 0 26px;font-size:15.5px;border-left:3px solid #14707f}\n.upl-page .faq h3{border-top:1px solid #eceff1;padding-top:22px;margin-top:0;font-size:18px}\n.upl-page .faq h3:first-of-type{border-top:0;padding-top:0}\n.upl-page .cta{background:linear-gradient(135deg,#0b2b33,#0d5563);color:#fff;border-radius:12px;padding:36px;margin:52px 0 20px}\n.upl-page .cta h2{color:#fff;margin:0 0 10px;font-size:25px}\n.upl-page .cta p{color:#c9dee3;margin:0 0 22px;font-size:16px}\n.upl-page .btn{display:inline-block;background:#e07a1f;color:#fff;text-decoration:none;font-weight:700;padding:13px 26px;border-radius:8px;font-size:15.5px}\n@media(max-width:640px){.upl-page h1{font-size:28px}.upl-page h2{font-size:22px}.upl-page .prod img{height:180px}.upl-page table{font-size:13px}}\n<\/style>\n<div class=\"upl-page\">\n<p class=\"lead\">Polycarbonate is what you specify when a part has to be transparent and survive being hit. It carries roughly 200 times the impact energy of glass at a fraction of the weight, holds clarity up to 120 \u00b0C, and takes a flame-retardant grade without turning opaque. The trade-off is that it is fussy about moisture and needs a hot mould \u2014 both of which are process disciplines, not material limits.<\/p>\n<p>  <img decoding=\"async\" src=\"https:\/\/uplastech.com\/wp-content\/uploads\/2026\/10\/polycarbonate-parts.jpg\" alt=\"Custom PC Injection Molding \u2014 Machine guards and transparent covers\" style=\"width:100%;border-radius:12px;margin:0 0 30px\"><\/p>\n<div class=\"stats\">\n<div class=\"stat\"><b>125 \u2013 135 \u00b0C<\/b><span>HDT at 1.8 MPa<\/span><\/div>\n<div class=\"stat\"><b>60 \u2013 70 MPa<\/b><span>Tensile strength<\/span><\/div>\n<div class=\"stat\"><b>1.20 g\/cm\u00b3<\/b><span>Densidad<\/span><\/div>\n<\/p><\/div>\n<p class=\"sec-note\">Typical values for standard moulding grades. Exact figures depend on the specific compound or grade \u2014 confirm against your drawing before quoting.<\/p>\n<h2>Key properties<\/h2>\n<table>\n<thead>\n<tr>\n<th>Propiedad<\/th>\n<th>Typical value<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>Densidad<\/td>\n<td>1.20 g\/cm\u00b3<\/td>\n<\/tr>\n<tr>\n<td>Tensile strength<\/td>\n<td>60 \u2013 70 MPa<\/td>\n<\/tr>\n<tr>\n<td>Flexural modulus<\/td>\n<td>2.3 \u2013 2.4 GPa<\/td>\n<\/tr>\n<tr>\n<td>HDT at 1.8 MPa<\/td>\n<td>125 \u2013 135 \u00b0C<\/td>\n<\/tr>\n<tr>\n<td>Mould shrinkage<\/td>\n<td>0.5 \u2013 0.7 %<\/td>\n<\/tr>\n<tr>\n<td>Light transmission<\/td>\n<td>88 \u2013 90 % at 3 mm<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p class=\"tablecap\">Values are typical for unfilled moulding grades at 23 \u00b0C unless stated. Glass-filled and specialty grades differ.<\/p>\n<h2>Typical applications<\/h2>\n<ul>\n<li>Machine guards and transparent covers<\/li>\n<li>LED light diffusers and lenses<\/li>\n<li>Medical device housings and fluid paths<\/li>\n<li>Safety helmets and protective visors<\/li>\n<li>Electrical enclosures requiring flame retardancy<\/li>\n<\/ul>\n<h2>Processing notes<\/h2>\n<ul>\n<li>Dry 4 h at 120 \u00b0C. This is not optional \u2014 0.02 % residual moisture is enough to hydrolyse the melt and drop impact strength by half.<\/li>\n<li>Melt 280 \u2013 310 \u00b0C, mould 80 \u2013 110 \u00b0C. A cold mould locks in stress and produces parts that craze weeks later.<\/li>\n<li>Annealing at 110 \u2013 120 \u00b0C for 1 \u2013 2 h relieves moulded-in stress where the part will meet solvents or sustained load.<\/li>\n<li>Gate away from high-stress zones and avoid sharp internal corners; PC notches rather than yields.<\/li>\n<\/ul>\n<div class=\"callout\">\n    <strong>Tooling, not just material.<\/strong> Every material above behaves differently in the tool \u2014 shrinkage, gate position, cooling and ejection all change. We review the DFM against the specific grade before the tool is cut, so the first shot is a sample, not a surprise.\n  <\/div>\n<div class=\"faq\">\n<h2>Frequently asked questions<\/h2>\n<h3>Will the part stay clear after years outdoors?<\/h3>\n<p>Standard PC yellows under UV. For outdoor clarity we specify a UV-coated grade or add a hard-coat after moulding. If the part is purely structural, an opaque PC\/ABS blend is cheaper and tougher at the edges.<\/p>\n<h3>Can PC be overmoulded with a soft-touch material?<\/h3>\n<p>Yes, with a TPE or TPU grade formulated for PC adhesion. The PC insert needs to be dry and the bond improves markedly if the insert is preheated to around 80 \u00b0C.<\/p>\n<\/p><\/div>\n<h2>Related materials<\/h2>\n<ul class=\"related\">\n<li><a href=\"\/es\/abs-injection-molding\/\">ABS Injection Molding<\/a><\/li>\n<li><a href=\"\/es\/pp-injection-molding\/\">PP Injection Molding<\/a><\/li>\n<li><a href=\"\/es\/pe-injection-molding\/\">PE Injection Molding<\/a><\/li>\n<li><a href=\"\/es\/nylon-pa-injection-molding\/\">Nylon Injection Molding<\/a><\/li>\n<li><a href=\"\/es\/pom-acetal-injection-molding\/\">POM Injection Molding<\/a><\/li>\n<li><a href=\"\/es\/acrylic-pmma-injection-molding\/\">PMMA Acrylic Injection Molding<\/a><\/li>\n<\/ul>\n<p><a href=\"\/es\/injection-molding\/\">\u2190 All Injection Molding Solutions<\/a><\/p>\n<div class=\"cta\">\n<h2>Send us your PC drawing<\/h2>\n<p>Upload a 3D model or a 2D drawing and we will come back with a DFM review, a tooling cost and a piece price \u2014 usually within two working days.<\/p>\n<p>    <a class=\"btn\" href=\"\/es\/pongase-en-contacto-con\/\">Request a quote<\/a>\n  <\/div>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>Polycarbonate is what you specify when a part has to be transparent and survive being hit. It carries roughly 200 times the impact energy of glass at a fraction of the weight, holds clarity up to 120 \u00b0C, and takes a flame-retardant grade without turning opaque. The trade-off is that it is fussy about moisture [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":0,"parent":0,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"","meta":{"_seopress_titles_title":"Custom PC Injection Molding | Uplastech","_seopress_titles_desc":"Custom polycarbonate injection moulding for transparent covers, light diffusers and impact-resistant housings. Optical clarity with high heat resistance.","_seopress_robots_index":"","_seopress_robots_follow":"","_seopress_robots_imageindex":"","_seopress_robots_snippet":"","_seopress_robots_primary_cat":"","_seopress_robots_breadcrumbs":"","_seopress_robots_freeze_modified_date":"","_seopress_robots_custom_modified_date":"","_seopress_robots_canonical":"","_seopress_social_fb_title":"","_seopress_social_fb_desc":"","_seopress_social_fb_img":"","_seopress_social_fb_img_attachment_id":0,"_seopress_social_fb_img_width":0,"_seopress_social_fb_img_height":0,"_seopress_social_twitter_title":"","_seopress_social_twitter_desc":"","_seopress_social_twitter_img":"","_seopress_social_twitter_img_attachment_id":0,"_seopress_social_twitter_img_width":0,"_seopress_social_twitter_img_height":0,"_seopress_redirections_value":"","_seopress_redirections_enabled":"","_seopress_redirections_enabled_regex":"","_seopress_redirections_logged_status":"","_seopress_redirections_param":"","_seopress_redirections_type":0,"_seopress_analysis_target_kw":"","footnotes":""},"class_list":["post-7320","page","type-page","status-publish","hentry"],"meta_box":[],"_links":{"self":[{"href":"https:\/\/uplastech.com\/es\/wp-json\/wp\/v2\/pages\/7320","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/uplastech.com\/es\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/uplastech.com\/es\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/uplastech.com\/es\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/uplastech.com\/es\/wp-json\/wp\/v2\/comments?post=7320"}],"version-history":[{"count":1,"href":"https:\/\/uplastech.com\/es\/wp-json\/wp\/v2\/pages\/7320\/revisions"}],"predecessor-version":[{"id":7375,"href":"https:\/\/uplastech.com\/es\/wp-json\/wp\/v2\/pages\/7320\/revisions\/7375"}],"wp:attachment":[{"href":"https:\/\/uplastech.com\/es\/wp-json\/wp\/v2\/media?parent=7320"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}